EN 12164 Grade CuNi12Zn30Pb1 R420

View suppliers (2)
Want to keep this datasheet? Save it now in your required format

Description

Material CuNi12Zn30Pb1, mat. No. CW406J is an alloy of high strength and hardness. To the comparabel mark CuNi12Zn30Pb1, mat. No. 2.0780, acc. to DIN 17663 : 1983-12 applies: Strength is further increasable due to the high strain hardening capability. The material does not embrittle at low temperatures. Low electrical and thermal conductivity. The alloy is non-magnetic, corrosion resistance is better than for pure copper. Machinability improves by Pb-addition, ductility decreases and cold workabiliy deteriorates. Processing properties: warm forming: unfavorable cold forming: moderately machinability: good hard and soft soldering: very good TIG-welding: moderately burnishing: good Application: Particularly in precision engineering and in toolbuilding for turning and drilling parts, in electrical engineering and electronics as well as in shipbuilding and in construction trade.

Related Standards

Diese Materialdaten wurden von WIAM zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Eigenschaften

Allgemein

PropertyTemperatureValue

Dichte

20.0 °C

8.6 - 8.62 g/cm³

Show Material materials with Dichte of 8.6 - 8.62 g/cm³

Mechanisch

PropertyTemperatureValueComment

Dehnung

20.0 °C

20 %

Show Material materials with Dehnung of 20 %

Elastizitätsmodul

20.0 °C

120 GPa

Show Material materials with Elastizitätsmodul of 120 GPa

Elongation A10

20.0 °C

16 %

Show Material materials with Elongation A10 of 16 %

Elongation A100

20.0 °C

12 %

Show Material materials with Elongation A100 of 12 %

Elongation A11.3

20.0 °C

16 %

Show Material materials with Elongation A11.3 of 16 %

Poissonzahl

23.0 °C

0.32 [-]

Show Material materials with Poissonzahl of 0.32 [-]

Typical for Wrought Copper Nickel Silver Grade

Streckgrenze Rp 0,2

20.0 °C

260 - 280 MPa

Show Material materials with Streckgrenze Rp 0,2 of 260 - 280 MPa

Zugfestigkeit

20.0 °C

420 MPa

Show Material materials with Zugfestigkeit of 420 MPa

Thermisch

PropertyTemperatureValueComment

Koeffizient der thermischen Ausdehnung

300.0 °C

1.95E-5 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 1.95E-5 1/K

Schmelzpunkt

875 - 1135 °C

Show Material materials with Schmelzpunkt of 875 - 1135 °C

Typical for Wrought Copper Nickel Silver Grade

Spezifische Wärmekapazität

23.0 °C

377 J/(kg·K)

Show Material materials with Spezifische Wärmekapazität of 377 J/(kg·K)

Typical for Wrought Copper Nickel Silver Grade

Wärmeleitfähigkeit

20.0 °C

42 W/(m·K)

Show Material materials with Wärmeleitfähigkeit of 42 W/(m·K)

Elektrisch

PropertyTemperatureValue

Elektrische Leitfähigkeit

20.0 °C

4.20E+6 S/m

Show Material materials with Elektrische Leitfähigkeit of 4.20E+6 S/m

Specific Electrical conductivity

7 % IACS

Show Material materials with Specific Electrical conductivity of 7 % IACS

Chemical properties

PropertyValue

Blei

0.5 - 1.5 %

Show Material materials with Blei of 0.5 - 1.5 %

Eisen

0.3 %

Show Material materials with Eisen of 0.3 %

Kupfer

56 - 58 %

Show Material materials with Kupfer of 56 - 58 %

Mangan

0.5 %

Show Material materials with Mangan of 0.5 %

Nickel

11 - 13 %

Show Material materials with Nickel of 11 - 13 %

Zinn

0.2 %

Show Material materials with Zinn of 0.2 %