Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.7 - 8.74 g/cm³ Show Material materials with Dichte of 8.7 - 8.74 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 20.0 °C | 130 GPa Show Material materials with Elastizitätsmodul of 130 GPa | |
Poissonzahl | 23.0 °C | 0.32 [-] Show Material materials with Poissonzahl of 0.32 [-] | Typical for Wrought Copper Nickel Silver Grade |
Streckgrenze Rp 0,2 | 20.0 °C | 580 - 600 MPa Show Material materials with Streckgrenze Rp 0,2 of 580 - 600 MPa | |
Zugfestigkeit | 20.0 °C | 650 MPa Show Material materials with Zugfestigkeit of 650 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 300.0 °C | 1.7E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.7E-5 1/K | |
Schmelzpunkt | 875 - 1135 °C Show Material materials with Schmelzpunkt of 875 - 1135 °C | Typical for Wrought Copper Nickel Silver Grade | |
Spezifische Wärmekapazität | 23.0 °C | 377 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 377 J/(kg·K) | Typical for Wrought Copper Nickel Silver Grade |
Wärmeleitfähigkeit | 20.0 °C | 33 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 33 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 3.20E+6 S/m Show Material materials with Elektrische Leitfähigkeit of 3.20E+6 S/m |
Specific Electrical conductivity | 5 % IACS Show Material materials with Specific Electrical conductivity of 5 % IACS |
Chemical properties
Property | Value |
---|---|
Blei | 0.5 - 1.5 % Show Material materials with Blei of 0.5 - 1.5 % |
Eisen | 0.3 % Show Material materials with Eisen of 0.3 % |
Kupfer | 59.5 - 62.5 % Show Material materials with Kupfer of 59.5 - 62.5 % |
Mangan | 0.7 % Show Material materials with Mangan of 0.7 % |
Nickel | 17 - 19 % Show Material materials with Nickel of 17 - 19 % |
Zinn | 0.2 % Show Material materials with Zinn of 0.2 % |