Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 8 % Show Material materials with Dehnung of 8 % | |
Elastizitätsmodul | 23.0 °C | 110 - 130 GPa Show Material materials with Elastizitätsmodul of 110 - 130 GPa | Typical for Wrought Copper High Copper Alloy |
Elongation A10 | 20.0 °C | 7 % Show Material materials with Elongation A10 of 7 % | |
Elongation A100 | 20.0 °C | 3 - 5 % Show Material materials with Elongation A100 of 3 - 5 % | |
Härte, Vickers | 20.0 °C | 350 - 410 [-] Show Material materials with Härte, Vickers of 350 - 410 [-] | |
Streckgrenze Rp 0,2 | 20.0 °C | 1050 - 1090 MPa Show Material materials with Streckgrenze Rp 0,2 of 1050 - 1090 MPa | |
Zugfestigkeit | 20.0 °C | 1100 - 1350 MPa Show Material materials with Zugfestigkeit of 1100 - 1350 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.6E-5 - 1.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 - 1.8E-5 1/K | Typical for Wrought Copper High Copper Alloy |
Schmelzpunkt | 855 - 1090 °C Show Material materials with Schmelzpunkt of 855 - 1090 °C | Typical for Wrought Copper High Copper Alloy | |
Spezifische Wärmekapazität | 23.0 °C | 360 - 420 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 360 - 420 J/(kg·K) | Typical for Wrought Copper High Copper Alloy |
Chemical properties
Property | Value |
---|---|
Beryllium | 1.8 - 2 % Show Material materials with Beryllium of 1.8 - 2 % |
Blei | 0.2 - 0.6 % Show Material materials with Blei of 0.2 - 0.6 % |
Eisen | 0.2 % Show Material materials with Eisen of 0.2 % |
Kobalt | 0.3 % Show Material materials with Kobalt of 0.3 % |
Nickel | 0.3 % Show Material materials with Nickel of 0.3 % |