Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 1 - 2 % Show Material materials with Dehnung of 1 - 2 % |
Härte, Vickers | 20.0 °C | 360 - 460 [-] Show Material materials with Härte, Vickers of 360 - 460 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 1150 - 1300 MPa Show Material materials with Streckgrenze Rp 0,2 of 1150 - 1300 MPa |
Zugfestigkeit | 20.0 °C | 1190 - 1520 MPa Show Material materials with Zugfestigkeit of 1190 - 1520 MPa |
Chemical properties
Property | Value |
---|---|
Beryllium | 1.8 - 2 % Show Material materials with Beryllium of 1.8 - 2 % |
Blei | 0.2 - 0.6 % Show Material materials with Blei of 0.2 - 0.6 % |
Eisen | 0.2 % Show Material materials with Eisen of 0.2 % |
Kobalt | 0.3 % Show Material materials with Kobalt of 0.3 % |
Nickel | 0.3 % Show Material materials with Nickel of 0.3 % |