Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.7 - 8.7 g/cm³ Show Material materials with Dichte of 7.7 - 8.7 g/cm³ | Typical for Leaded Phosphor Bronze |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 20 % Show Material materials with Dehnung of 20 % | |
Elastizitätsmodul | 23.0 °C | 110 - 130 GPa Show Material materials with Elastizitätsmodul of 110 - 130 GPa | Typical for Leaded Phosphor Bronze |
Elongation A10 | 20.0 °C | 17 % Show Material materials with Elongation A10 of 17 % | |
Elongation A100 | 20.0 °C | 15 % Show Material materials with Elongation A100 of 15 % | |
Poissonzahl | 23.0 °C | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Leaded Phosphor Bronze |
Streckgrenze Rp 0,2 | 20.0 °C | 200 MPa Show Material materials with Streckgrenze Rp 0,2 of 200 MPa | |
Zugfestigkeit | 20.0 °C | 410 - 510 MPa Show Material materials with Zugfestigkeit of 410 - 510 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.5E-5 - 1.9E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.5E-5 - 1.9E-5 1/K | Typical for Leaded Phosphor Bronze |
Spezifische Wärmekapazität | 23.0 °C | 380 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 380 J/(kg·K) | Typical for Leaded Phosphor Bronze |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.02 % Show Material materials with Aluminium of 0.02 % |
Blei | 0.05 % Show Material materials with Blei of 0.05 % |
Eisen | 0.8 % Show Material materials with Eisen of 0.8 % |
Mangan | 0.7 % Show Material materials with Mangan of 0.7 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Silizium | 0.8 - 2 % Show Material materials with Silizium of 0.8 - 2 % |
Zink | 1.5 % Show Material materials with Zink of 1.5 % |