Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.8 - 8.9 g/cm³ Show Material materials with Dichte of 8.8 - 8.9 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 20.0 °C | 120 GPa Show Material materials with Elastizitätsmodul of 120 GPa | |
Härte, Vickers | 20.0 °C | 110 - 140 [-] Show Material materials with Härte, Vickers of 110 - 140 [-] | |
Poissonzahl | 23.0 °C | 0.34 [-] Show Material materials with Poissonzahl of 0.34 [-] | Typical for Wrought Copper Pure / Low Alloyed Copper |
Schubmodule | 23.0 °C | 48 GPa Show Material materials with Schubmodule of 48 GPa | Typical for Wrought Copper Pure / Low Alloyed Copper |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 300.0 °C | 1.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.8E-5 1/K | |
Schmelzpunkt | 965 - 1100 °C Show Material materials with Schmelzpunkt of 965 - 1100 °C | Typical for Wrought Copper Pure / Low Alloyed Copper | |
Spezifische Wärmekapazität | 23.0 °C | 377 - 420 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 377 - 420 J/(kg·K) | Typical for Wrought Copper Pure / Low Alloyed Copper |
Wärmeleitfähigkeit | 20.0 °C | 368 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 368 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 5.45E+7 S/m Show Material materials with Elektrische Leitfähigkeit of 5.45E+7 S/m |
Chemical properties
Property | Value |
---|---|
Phosphor | 0 - 0.01 % Show Material materials with Phosphor of 0 - 0.01 % |
Tellur | 0.4 - 0.7 % Show Material materials with Tellur of 0.4 - 0.7 % |