Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.55 g/cm³ Show Material materials with Dichte of 8.55 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 100 - 125 GPa Show Material materials with Elastizitätsmodul of 100 - 125 GPa | Typical for Wrought Copper Brass |
Elongation A10 | 20.0 °C | 10 % Show Material materials with Elongation A10 of 10 % | |
Elongation A100 | 20.0 °C | 7 % Show Material materials with Elongation A100 of 7 % | |
Härte, Vickers | 20.0 °C | 120 - 160 [-] Show Material materials with Härte, Vickers of 120 - 160 [-] | |
Schubmodule | 23.0 °C | 40 GPa Show Material materials with Schubmodule of 40 GPa | Typical for Wrought Copper Brass |
Streckgrenze Rp 0,2 | 20.0 °C | 290 - 340 MPa Show Material materials with Streckgrenze Rp 0,2 of 290 - 340 MPa | |
Zugfestigkeit | 20.0 °C | 440 - 620 MPa Show Material materials with Zugfestigkeit of 440 - 620 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 150.0 °C | 1.9E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.9E-5 1/K | |
300.0 °C | 2E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2E-5 1/K | ||
Schmelzpunkt | 875 - 1075 °C Show Material materials with Schmelzpunkt of 875 - 1075 °C | Typical for Wrought Copper Brass | |
Spezifische Wärmekapazität | 20.0 °C | 377 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 377 J/(kg·K) | |
Wärmeleitfähigkeit | -200.0 °C | 50 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 50 W/(m·K) | |
20.0 °C | 121 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 121 W/(m·K) | ||
200.0 °C | 147 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 147 W/(m·K) | ||
Chemical properties
Property | Value |
---|---|
Aluminium | 0.02 % Show Material materials with Aluminium of 0.02 % |
Blei | 0.05 % Show Material materials with Blei of 0.05 % |
Eisen | 0.05 % Show Material materials with Eisen of 0.05 % |
Kupfer | 69 - 71 % Show Material materials with Kupfer of 69 - 71 % |
Nickel | 0.3 % Show Material materials with Nickel of 0.3 % |
Zinn | 0.1 % Show Material materials with Zinn of 0.1 % |