Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 8 % Show Material materials with Dehnung of 8 % | |
Elastizitätsmodul | 23.0 °C | 100 - 125 GPa Show Material materials with Elastizitätsmodul of 100 - 125 GPa | Typical for Wrought Copper Brass |
Elongation A10 | 20.0 °C | 6 % Show Material materials with Elongation A10 of 6 % | |
Elongation A100 | 20.0 °C | 4 % Show Material materials with Elongation A100 of 4 % | |
Härte, Vickers | 20.0 °C | 145 - 185 [-] Show Material materials with Härte, Vickers of 145 - 185 [-] | |
Schubmodule | 23.0 °C | 40 GPa Show Material materials with Schubmodule of 40 GPa | Typical for Wrought Copper Brass |
Streckgrenze Rp 0,2 | 20.0 °C | 390 - 400 MPa Show Material materials with Streckgrenze Rp 0,2 of 390 - 400 MPa | |
Zugfestigkeit | 20.0 °C | 490 - 520 MPa Show Material materials with Zugfestigkeit of 490 - 520 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.7E-5 - 2.1E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.7E-5 - 2.1E-5 1/K | Typical for Wrought Copper Brass |
Schmelzpunkt | 875 - 1075 °C Show Material materials with Schmelzpunkt of 875 - 1075 °C | Typical for Wrought Copper Brass | |
Spezifische Wärmekapazität | 23.0 °C | 371 - 418 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 371 - 418 J/(kg·K) | Typical for Wrought Copper Brass |
Wärmeleitfähigkeit | 23.0 °C | 100 - 234 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 100 - 234 W/(m·K) | Typical for Wrought Copper Brass |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 % Show Material materials with Aluminium of 0.05 % |
Blei | 3.5 - 4.2 % Show Material materials with Blei of 3.5 - 4.2 % |
Eisen | 0.3 % Show Material materials with Eisen of 0.3 % |
Kupfer | 57 - 59 % Show Material materials with Kupfer of 57 - 59 % |
Nickel | 0.3 % Show Material materials with Nickel of 0.3 % |
Zinn | 0.3 % Show Material materials with Zinn of 0.3 % |