EN 12167 Grade CuCo2Be H220

View suppliers (3)
Want to keep this datasheet? Save it now in your required format

Description

Cuco2Be, mat. No CW104C, is counted among hardenable, low alloyed copper alloys. To the comparable make Cuco2Be, mat. No 2.1285, acc. to DIN 17666 : 1983-12 applies: CuCo2Be achieves compared to CuBe2 at slightly lower hardness and strength values higher electrical and thermal conductivity. The temperature for removal of workhardening approximates 500°C, high corrosion resistance. Processing properties: hot and cold forming: good machinability: moderately hard and soft soldering: good gas shielded welding: good burnishing: good Application: In relay and switch construction for high loadable, live springs and for radiant heaters at semi conductors. Furthermore for resistance and welding electrodes as well as for pistons, plunger and punching tools. For the electrolytically tinned strip the coatings (Sn bright, Sn matt, Sn fuzed, SnPb) are listed by the application (better solderability, better corrosion resistance, reduction of the electrical contact resistance, better appearance) in the DIN EN 14436 : 2004-11 (Table 5)

Related Standards

Equivalent Materials

Diese Materialdaten wurden von WIAM zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Eigenschaften

Allgemein

PropertyTemperatureValue

Dichte

20.0 °C

8.8 - 8.9 g/cm³

Show Material materials with Dichte of 8.8 - 8.9 g/cm³

Mechanisch

PropertyTemperatureValue

Elastizitätsmodul

20.0 °C

138 GPa

Show Material materials with Elastizitätsmodul of 138 GPa

Härte, Brinell

20.0 °C

220 - 270 [-]

Show Material materials with Härte, Brinell of 220 - 270 [-]

Thermisch

PropertyTemperatureValueComment

Koeffizient der thermischen Ausdehnung

300.0 °C

1.8E-5 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 1.8E-5 1/K

Max. Betriebstemperatur, lang

0 - 350 °C

Show Material materials with Max. Betriebstemperatur, lang of 0 - 350 °C

Schmelzpunkt

855 - 1090 °C

Show Material materials with Schmelzpunkt of 855 - 1090 °C

Typical for Wrought Copper High Copper Alloy

Spezifische Wärmekapazität

23.0 °C

360 - 420 J/(kg·K)

Show Material materials with Spezifische Wärmekapazität of 360 - 420 J/(kg·K)

Typical for Wrought Copper High Copper Alloy

Wärmeleitfähigkeit

20.0 °C

192 - 239 W/(m·K)

Show Material materials with Wärmeleitfähigkeit of 192 - 239 W/(m·K)

Elektrisch

PropertyTemperatureValue

Elektrische Leitfähigkeit

20.0 °C

2.50E+7 - 3.20E+7 S/m

Show Material materials with Elektrische Leitfähigkeit of 2.50E+7 - 3.20E+7 S/m

Specific Electrical conductivity

43 % IACS

Show Material materials with Specific Electrical conductivity of 43 % IACS

Chemical properties

PropertyValue

Beryllium

0.4 - 0.7 %

Show Material materials with Beryllium of 0.4 - 0.7 %

Eisen

0.2 %

Show Material materials with Eisen of 0.2 %

Kobalt

2 - 2.8 %

Show Material materials with Kobalt of 2 - 2.8 %

Nickel

0.3 %

Show Material materials with Nickel of 0.3 %