CuZr, mat. No CW120C, is counted among hardenable, low alloyed copper alloys. To the comparable make CuZr, mat. No 2.1580, acc. to DIN 17666 : 1983-12 applies: The strength properties of CuZr are not as favorable as for CuCrZr but it very well meets high requirements to tempering strength and creep strength at preferably high electric conductivity.Temperature for removal of workhardening approximates 525°C. Processing properties: hot and cold forming: good machinability: moderately soft soldering: moderately hard soldering: moderately gas shielded welding: moderately burnishing: good Application: For commutator lamellae of high strains, rotor windings in high loaded electric motors, diode bases, resistance welding electrodes as well as for electronic calculators.

Related Standards

Equivalent Materials

Diese Materialdaten wurden von WIAM zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Eigenschaften

Allgemein

PropertyTemperatureValue

Dichte

20.0 °C

8.9 g/cm³

Show Material materials with Dichte of 8.9 g/cm³

Mechanisch

PropertyTemperatureValueComment

Elastizitätsmodul

20.0 °C

135 GPa

Show Material materials with Elastizitätsmodul of 135 GPa

Härte, Brinell

20.0 °C

120 - 160 [-]

Show Material materials with Härte, Brinell of 120 - 160 [-]

Poissonzahl

23.0 °C

0.34 [-]

Show Material materials with Poissonzahl of 0.34 [-]

Typical for Wrought Copper Pure / Low Alloyed Copper

Schubmodule

23.0 °C

48 GPa

Show Material materials with Schubmodule of 48 GPa

Typical for Wrought Copper Pure / Low Alloyed Copper

Thermisch

PropertyTemperatureValueComment

Koeffizient der thermischen Ausdehnung

300.0 °C

1.7E-5 - 1.8E-5 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 1.7E-5 - 1.8E-5 1/K

Schmelzpunkt

965 - 1100 °C

Show Material materials with Schmelzpunkt of 965 - 1100 °C

Typical for Wrought Copper Pure / Low Alloyed Copper

Spezifische Wärmekapazität

23.0 °C

377 - 420 J/(kg·K)

Show Material materials with Spezifische Wärmekapazität of 377 - 420 J/(kg·K)

Typical for Wrought Copper Pure / Low Alloyed Copper

Wärmeleitfähigkeit

20.0 °C

167 - 330 W/(m·K)

Show Material materials with Wärmeleitfähigkeit of 167 - 330 W/(m·K)

Elektrisch

PropertyTemperatureValue

Elektrische Leitfähigkeit

20.0 °C

2.60E+7 - 5.40E+7 S/m

Show Material materials with Elektrische Leitfähigkeit of 2.60E+7 - 5.40E+7 S/m

Specific Electrical conductivity

86 % IACS

Show Material materials with Specific Electrical conductivity of 86 % IACS

Chemical properties

PropertyValue

Zirkonium

0.1 - 0.2 %

Show Material materials with Zirkonium of 0.1 - 0.2 %