Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.55 g/cm³ Show Material materials with Dichte of 8.55 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 45 % Show Material materials with Dehnung of 45 % | |
Elastizitätsmodul | 23.0 °C | 100 - 125 GPa Show Material materials with Elastizitätsmodul of 100 - 125 GPa | Typical for Wrought Copper Brass |
Härte, Vickers | 20.0 °C | 75 - 105 [-] Show Material materials with Härte, Vickers of 75 - 105 [-] | |
Schubmodule | 23.0 °C | 40 GPa Show Material materials with Schubmodule of 40 GPa | Typical for Wrought Copper Brass |
Streckgrenze Rp 0,2 | 20.0 °C | 130 MPa Show Material materials with Streckgrenze Rp 0,2 of 130 MPa | |
Zugfestigkeit | 20.0 °C | 340 MPa Show Material materials with Zugfestigkeit of 340 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.7E-5 - 2.1E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.7E-5 - 2.1E-5 1/K | Typical for Wrought Copper Brass |
Schmelzpunkt | 875 - 1075 °C Show Material materials with Schmelzpunkt of 875 - 1075 °C | Typical for Wrought Copper Brass | |
Spezifische Wärmekapazität | 23.0 °C | 371 - 418 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 371 - 418 J/(kg·K) | Typical for Wrought Copper Brass |
Wärmeleitfähigkeit | 20.0 °C | 126 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 126 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 1.63E+7 S/m Show Material materials with Elektrische Leitfähigkeit of 1.63E+7 S/m |
Specific Electrical conductivity | 28 % IACS Show Material materials with Specific Electrical conductivity of 28 % IACS |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.02 % Show Material materials with Aluminium of 0.02 % |
Arsen | 0.02 - 0.06 % Show Material materials with Arsen of 0.02 - 0.06 % |
Blei | 0.07 % Show Material materials with Blei of 0.07 % |
Eisen | 0.05 % Show Material materials with Eisen of 0.05 % |
Kupfer | 69 - 71 % Show Material materials with Kupfer of 69 - 71 % |
Mangan | 0.1 % Show Material materials with Mangan of 0.1 % |
Phosphor | 0.01 % Show Material materials with Phosphor of 0.01 % |
Zinn | 0.05 % Show Material materials with Zinn of 0.05 % |