Allgemein
Property | Value | Condition |
---|---|---|
Dichte | 5.0 g/cm³ Show Material materials with Dichte of 5.0 g/cm³ | Moderate Strength |
Mechanisch
Property | Value | Condition |
---|---|---|
Dehnung | 12.0 % Show Material materials with Dehnung of 12.0 % | Moderate Strength |
Elastizitätsmodul | 130.0 GPa Show Material materials with Elastizitätsmodul of 130.0 GPa | Moderate Strength |
Streckgrenze | 980.0 MPa Show Material materials with Streckgrenze of 980.0 MPa | Moderate Strength |
Zugfestigkeit | 1070.0 MPa Show Material materials with Zugfestigkeit of 1070.0 MPa | Moderate Strength |
Thermisch
Property | Value | Condition | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 9.6e-06 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 9.6e-06 1/K | Moderate Strength | |
Schmelzpunkt | 1550.0 - 1815.0 °C Show Material materials with Schmelzpunkt of 1550.0 - 1815.0 °C | Typical for Titanium Beta Alloy | |
Spezifische Wärmekapazität | 510.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 510.0 J/(kg·K) | Moderate Strength | |
Wärmeleitfähigkeit | 6.0 - 11.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 6.0 - 11.0 W/(m·K) | Typical for Titanium Beta Alloy |
Chemical properties
Property | Value | Condition |
---|---|---|
Aluminium | 3.0 - 4.0 % Show Material materials with Aluminium of 3.0 - 4.0 % | Moderate Strength |
Andere | 0.4 % Show Material materials with Andere of 0.4 % | Moderate Strength |
Chrom | 5.5 - 6.5 % Show Material materials with Chrom of 5.5 - 6.5 % | Moderate Strength |
Eisen | 0.3 % Show Material materials with Eisen of 0.3 % | Moderate Strength |
Kohlenstoff | 0.05 % Show Material materials with Kohlenstoff of 0.05 % | Moderate Strength |
Molybdän | 3.5 - 4.5 % Show Material materials with Molybdän of 3.5 - 4.5 % | Moderate Strength |
Palladium | 0.04 - 0.08 % Show Material materials with Palladium of 0.04 - 0.08 % | Moderate Strength |
Sauerstoff | 0.12 % Show Material materials with Sauerstoff of 0.12 % | Moderate Strength |
Stickstoff | 0.03 % Show Material materials with Stickstoff of 0.03 % | Moderate Strength |
Titan | 71.0 - 77.0 % Show Material materials with Titan of 71.0 - 77.0 % | Moderate Strength |
Vanadium | 7.5 - 8.5 % Show Material materials with Vanadium of 7.5 - 8.5 % | Moderate Strength |
Wasserstoff | 0.02 % Show Material materials with Wasserstoff of 0.02 % | Moderate Strength |
Zirkonium | 3.5 - 4.5 % Show Material materials with Zirkonium of 3.5 - 4.5 % | Moderate Strength |