Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 10 g/cm³ Show Material materials with Dichte of 10 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 12 % Show Material materials with Dehnung of 12 % | |
Elastizitätsmodul | 23.0 °C | 330 GPa Show Material materials with Elastizitätsmodul of 330 GPa | |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Molybdenum |
Schubmodule | 23.0 °C | 125 GPa Show Material materials with Schubmodule of 125 GPa | Typical for Molybdenum |
Streckgrenze | 23.0 °C | 360 MPa Show Material materials with Streckgrenze of 360 MPa | |
Zugfestigkeit | 23.0 °C | 590 MPa Show Material materials with Zugfestigkeit of 590 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2E-5 1/K | |
Schmelzpunkt | 2610 °C Show Material materials with Schmelzpunkt of 2610 °C | Typical for Molybdenum | |
Spezifische Wärmekapazität | 23.0 °C | 250 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 250 J/(kg·K) | |
Wärmeleitfähigkeit | 23.0 °C | 117 - 431 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 117 - 431 W/(m·K) | Typical for Molybdenum |
Chemical properties
Property | Value |
---|---|
Eisen | 0 - 0.01 % Show Material materials with Eisen of 0 - 0.01 % |
Kohlenstoff | 0.01 - 0.03 % Show Material materials with Kohlenstoff of 0.01 - 0.03 % |
Molybdän | 99.3 - 99.5 % Show Material materials with Molybdän of 99.3 - 99.5 % |
Nickel | 0 - 2E-3 % Show Material materials with Nickel of 0 - 2E-3 % |
Sauerstoff | 0 - 3E-3 % Show Material materials with Sauerstoff of 0 - 3E-3 % |
Silizium | 0 - 0.01 % Show Material materials with Silizium of 0 - 0.01 % |
Stickstoff | 0 - 2E-3 % Show Material materials with Stickstoff of 0 - 2E-3 % |
Titan | 0.4 - 0.55 % Show Material materials with Titan of 0.4 - 0.55 % |
Zirkonium | 0.06 - 0.12 % Show Material materials with Zirkonium of 0.06 - 0.12 % |