Allgemein
Property | Value | Condition |
---|---|---|
Dichte | 4.4 g/cm³ Show Material materials with Dichte of 4.4 g/cm³ | Solution Treated |
Mechanisch
Property | Value | Condition |
---|---|---|
Dehnung | 8.7 % Show Material materials with Dehnung of 8.7 % | Solution Treated |
Elastizitätsmodul | 120.0 GPa Show Material materials with Elastizitätsmodul of 120.0 GPa | Solution Treated |
Streckgrenze | 1130.0 MPa Show Material materials with Streckgrenze of 1130.0 MPa | Solution Treated |
Zugfestigkeit | 1200.0 MPa Show Material materials with Zugfestigkeit of 1200.0 MPa | Solution Treated |
Thermisch
Property | Value | Condition |
---|---|---|
Koeffizient der thermischen Ausdehnung | 8.9e-06 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 8.9e-06 1/K | Solution Treated |
Schmelzpunkt | 1650.0 °C Show Material materials with Schmelzpunkt of 1650.0 °C | Solution Treated |
Spezifische Wärmekapazität | 560.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 560.0 J/(kg·K) | Solution Treated |
Wärmeleitfähigkeit | 6.8 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 6.8 W/(m·K) | Solution Treated |
Chemical properties
Property | Value | Condition |
---|---|---|
Aluminium | 5.5 - 6.8 % Show Material materials with Aluminium of 5.5 - 6.8 % | Solution Treated |
Andere | 0.4 % Show Material materials with Andere of 0.4 % | Solution Treated |
Eisen | 0.4 % Show Material materials with Eisen of 0.4 % | Solution Treated |
Kohlenstoff | 0.08 % Show Material materials with Kohlenstoff of 0.08 % | Solution Treated |
Sauerstoff | 0.2 % Show Material materials with Sauerstoff of 0.2 % | Solution Treated |
Stickstoff | 0.05 % Show Material materials with Stickstoff of 0.05 % | Solution Treated |
Titan | 87.4 - 91.0 % Show Material materials with Titan of 87.4 - 91.0 % | Solution Treated |
Vanadium | 3.5 - 4.5 % Show Material materials with Vanadium of 3.5 - 4.5 % | Solution Treated |
Wasserstoff | 0.015 % Show Material materials with Wasserstoff of 0.015 % | Solution Treated |
Yttrium | 0.005 % Show Material materials with Yttrium of 0.005 % | Solution Treated |