Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.26 - 8.8 g/cm³ Show Material materials with Dichte of 8.26 - 8.8 g/cm³ |
Abmessung
Property | Value |
---|---|
Außendurchmesser | 19.1 - 406 mm Show Material materials with Außendurchmesser of 19.1 - 406 mm |
Breite | 1.27 - 406.5 mm Show Material materials with Breite of 1.27 - 406.5 mm |
Dicke | 0.05 - 4.77 mm Show Material materials with Dicke of 0.05 - 4.77 mm |
Wall thickness | 10-20% of outside diameter |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefähigkeit 90°, in longitudinaler Richtung | 23.0 °C | 0 - 3.5 [-] Show Material materials with Biegefähigkeit 90°, in longitudinaler Richtung of 0 - 3.5 [-] | for strip with 0.20mm and thinner.,for strip with 0.25mm and thinner. |
Biegefähigkeit 90°, in transversaler Richtung | 23.0 °C | 0 - 3 [-] Show Material materials with Biegefähigkeit 90°, in transversaler Richtung of 0 - 3 [-] | for strip with 0.20mm and thinner.,for strip with 0.25mm and thinner. |
Dehnung | 23.0 °C | 1 - 75 % Show Material materials with Dehnung of 1 - 75 % | min., for strip thicker than 0.10 mm,for wire with 0.1mm diameter and more. |
Elastizitätsmodul | 23.0 °C | 130 - 131 GPa Show Material materials with Elastizitätsmodul of 130 - 131 GPa | |
Härte, Rockwell C | 23.0 °C | 36 - 42 [-] Show Material materials with Härte, Rockwell C of 36 - 42 [-] | |
Härte, Vickers | 23.0 °C | 210 - 446 [-] Show Material materials with Härte, Vickers of 210 - 446 [-] | |
Schubmodule | 23.0 °C | 50 GPa Show Material materials with Schubmodule of 50 GPa | |
Streckgrenze | 23.0 °C | 220 MPa Show Material materials with Streckgrenze of 220 MPa | |
Streckgrenze Rp 0,2 | 23.0 °C | 130 - 1420 MPa Show Material materials with Streckgrenze Rp 0,2 of 130 - 1420 MPa | |
Zugfestigkeit | 23.0 °C | 410 - 1520 MPa Show Material materials with Zugfestigkeit of 410 - 1520 MPa | min. |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.75E-5 - 1.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.75E-5 - 1.8E-5 1/K |
Schmelzpunkt | 870 °C Show Material materials with Schmelzpunkt of 870 °C | |
Spezifische Wärmekapazität | 23.0 °C | 360 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 360 J/(kg·K) |
Wärmeleitfähigkeit | 23.0 °C | 84 - 130 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 84 - 130 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Specific Electrical conductivity | 17 - 30 % IACS Show Material materials with Specific Electrical conductivity of 17 - 30 % IACS | |
spezifischer Widerstand | 23.0 °C | 6.2E-8 - 7.8E-6 Ω·m Show Material materials with spezifischer Widerstand of 6.2E-8 - 7.8E-6 Ω·m |
Magnetisch
Property | Temperature | Value | Comment |
---|---|---|---|
Relative magnetische Permeabilität | 23.0 °C | 1 [-] Show Material materials with Relative magnetische Permeabilität of 1 [-] | max. |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0 - 0.2 % Show Material materials with Aluminium of 0 - 0.2 % | |
Andere | 0 - 0.6 % Show Material materials with Andere of 0 - 0.6 % | max., Co+Ni+Fe |
Beryllium | 1.8 - 2.2 % Show Material materials with Beryllium of 1.8 - 2.2 % | |
Blei | 0.2 - 0.6 % Show Material materials with Blei of 0.2 - 0.6 % | |
Eisen | 0 - 0.6 % Show Material materials with Eisen of 0 - 0.6 % | max., Nickel + Cobalt + Iron,max. Nickel + Cobalt + Iron |
Kobalt | 0.2 - 0.3 % Show Material materials with Kobalt of 0.2 - 0.3 % | max.,min. Nickel + Cobalt |
Kupfer | 96.1 - 98 % Show Material materials with Kupfer of 96.1 - 98 % | Balance |
Nickel | 0.2 - 0.6 % Show Material materials with Nickel of 0.2 - 0.6 % | min. Nickel + Cobalt |
Silizium | 0 - 0.2 % Show Material materials with Silizium of 0 - 0.2 % |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace: Landing gear, bearing bushes and high performance fasteners;Automotive: Valve guides, bushes and valve seats;Offshore & marine: Offshore drilling and instrumentation equipment, downhole tooling, valve, pump and shaft components;Other: Deep drawing tooling, plastic moulding dies, tools and plungers, die-casting plunger tips, non-magnetic and non sparking tools, electrical and electronic connectors, springs, fasteners, switchgear, resistance welding electrodes and equipment, flash butt welding dies and inserts, seam welding electrode shafts,Typical applications include high reliability spring contacts for battery contacts, audio jack contacts, and board to board contacts.,Typical applications include high reliability spring contacts for switches and relays, battery contacts, and automotive terminals.,Typical applications include bushings and bearings for aircraft as well as drill collars and instrument housings for oil and gas exploration.,Typical applications include pressure sensor bellows, burn-in and test socket contacts, computer processor socket contacts, and electromagnetic shielding gaskets.,EtchMet alloy is a material that is tailor made for the springs in voice coil motors and optical image stabilization systems common in smart phone cameras. | |
Corrosion properties | High corrosion resistance | |
General machinability | Very good machinability |