Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.41 - 8.8 g/cm³ Show Material materials with Dichte of 8.41 - 8.8 g/cm³ |
Abmessung
Property | Value | Comment |
---|---|---|
Außendurchmesser | 19.1 - 406 mm Show Material materials with Außendurchmesser of 19.1 - 406 mm | |
Breite | 305 - 559 mm Show Material materials with Breite of 305 - 559 mm | |
Dicke | 12.7 - 203.2 mm Show Material materials with Dicke of 12.7 - 203.2 mm | |
Durchmesser | 0.76 - 356 mm Show Material materials with Durchmesser of 0.76 - 356 mm | |
Länge | 610 - 91000 mm Show Material materials with Länge of 610 - 91000 mm | max. |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 7.8 - 75 % Show Material materials with Dehnung of 7.8 - 75 % |
Elastizitätsmodul | 23.0 °C | 120 - 131 GPa Show Material materials with Elastizitätsmodul of 120 - 131 GPa |
Streckgrenze | 23.0 °C | 600 MPa Show Material materials with Streckgrenze of 600 MPa |
Streckgrenze Rp 0,2 | 23.0 °C | 130 - 250 MPa Show Material materials with Streckgrenze Rp 0,2 of 130 - 250 MPa |
Zugfestigkeit | 23.0 °C | 410 - 750 MPa Show Material materials with Zugfestigkeit of 410 - 750 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.6E-5 - 1.75E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 - 1.75E-5 1/K |
Schmelzpunkt | 870 °C Show Material materials with Schmelzpunkt of 870 °C | |
Spezifische Wärmekapazität | 23.0 °C | 410 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 410 J/(kg·K) |
Wärmeleitfähigkeit | 23.0 °C | 105 - 110 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 105 - 110 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Specific Electrical conductivity | 25 - 30 % IACS Show Material materials with Specific Electrical conductivity of 25 - 30 % IACS | |
spezifischer Widerstand | 23.0 °C | 5.8E-6 - 6.9E-6 Ω·m Show Material materials with spezifischer Widerstand of 5.8E-6 - 6.9E-6 Ω·m |
Magnetisch
Property | Temperature | Value | Comment |
---|---|---|---|
Relative magnetische Permeabilität | 23.0 °C | 1 [-] Show Material materials with Relative magnetische Permeabilität of 1 [-] | max. |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0 - 0.2 % Show Material materials with Aluminium of 0 - 0.2 % | |
Andere | 0 - 0.5 % Show Material materials with Andere of 0 - 0.5 % | |
Beryllium | 1.6 - 1.85 % Show Material materials with Beryllium of 1.6 - 1.85 % | |
Eisen | 0 - 0.6 % Show Material materials with Eisen of 0 - 0.6 % | max., Nickel + Cobalt + Iron |
Kobalt | 0.2 % Show Material materials with Kobalt of 0.2 % | min. Nickel + Cobalt |
Kupfer | 96.3 - 98.2 % Show Material materials with Kupfer of 96.3 - 98.2 % | Balance |
Nickel | 0.2 - 0.6 % Show Material materials with Nickel of 0.2 - 0.6 % | min. Nickel + Cobalt |
Silizium | 0 - 0.2 % Show Material materials with Silizium of 0 - 0.2 % |
Technological properties
Property | ||
---|---|---|
Application areas | Alloy 165 tube is used in crucial telecommunications applications including undersea instrument housings and repeater housings.,Typical applications include bushings, bearings and resistance welding components.,Typical applications include wear plates and resistance welding components. |