Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.26 - 8.8 g/cm³ Show Material materials with Dichte of 8.26 - 8.8 g/cm³ |
Abmessung
Property | Value |
---|---|
Außendurchmesser | 9.5 - 76 mm Show Material materials with Außendurchmesser of 9.5 - 76 mm |
Breite | 305 - 559 mm Show Material materials with Breite of 305 - 559 mm |
Dicke | 12.7 - 203.2 mm Show Material materials with Dicke of 12.7 - 203.2 mm |
Länge | 610 - 3200 mm Show Material materials with Länge of 610 - 3200 mm |
Wall thickness | 10-20% of outside diameter |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 1 - 75 % Show Material materials with Dehnung of 1 - 75 % | for wire with 0.1mm diameter and more. |
Elastizitätsmodul | 23.0 °C | 130 - 131 GPa Show Material materials with Elastizitätsmodul of 130 - 131 GPa | |
Härte, Rockwell C | 23.0 °C | 37 - 45 [-] Show Material materials with Härte, Rockwell C of 37 - 45 [-] | |
Schubmodule | 23.0 °C | 50 GPa Show Material materials with Schubmodule of 50 GPa | |
Streckgrenze | 23.0 °C | 630 MPa Show Material materials with Streckgrenze of 630 MPa | |
Streckgrenze Rp 0,2 | 23.0 °C | 130 - 1380 MPa Show Material materials with Streckgrenze Rp 0,2 of 130 - 1380 MPa | |
Zugfestigkeit | 23.0 °C | 410 - 1550 MPa Show Material materials with Zugfestigkeit of 410 - 1550 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.75E-5 - 1.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.75E-5 - 1.8E-5 1/K |
Schmelzpunkt | 870 °C Show Material materials with Schmelzpunkt of 870 °C | |
Spezifische Wärmekapazität | 23.0 °C | 360 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 360 J/(kg·K) |
Wärmeleitfähigkeit | 23.0 °C | 84 - 130 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 84 - 130 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Specific Electrical conductivity | 22 - 30 % IACS Show Material materials with Specific Electrical conductivity of 22 - 30 % IACS | |
spezifischer Widerstand | 23.0 °C | 7.9E-8 - 7.8E-6 Ω·m Show Material materials with spezifischer Widerstand of 7.9E-8 - 7.8E-6 Ω·m |
Magnetisch
Property | Temperature | Value | Comment |
---|---|---|---|
Relative magnetische Permeabilität | 23.0 °C | 1 [-] Show Material materials with Relative magnetische Permeabilität of 1 [-] | max. |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0 - 0.2 % Show Material materials with Aluminium of 0 - 0.2 % | |
Andere | 0 - 0.6 % Show Material materials with Andere of 0 - 0.6 % | max., Co+Ni+Fe |
Beryllium | 1.8 - 2 % Show Material materials with Beryllium of 1.8 - 2 % | |
Blei | 0.2 - 0.6 % Show Material materials with Blei of 0.2 - 0.6 % | |
Eisen | 0 - 0.6 % Show Material materials with Eisen of 0 - 0.6 % | max., Nickel + Cobalt + Iron,max. Nickel + Cobalt + Iron |
Kobalt | 0.2 - 0.3 % Show Material materials with Kobalt of 0.2 - 0.3 % | min. Nickel + Cobalt,max. |
Kupfer | 96.1 - 98 % Show Material materials with Kupfer of 96.1 - 98 % | Balance |
Nickel | 0.2 - 0.6 % Show Material materials with Nickel of 0.2 - 0.6 % | min. Nickel + Cobalt |
Silizium | 0 - 0.2 % Show Material materials with Silizium of 0 - 0.2 % |
Technological properties
Property | ||
---|---|---|
Application areas | Typical applications include wear plates and other galling resistant components.,Aerospace: Landing gear, bearing bushes and high performance fasteners;Automotive: Valve guides, bushes and valve seats;Offshore & marine: Offshore drilling and instrumentation equipment, downhole tooling, valve, pump and shaft components;Other: Deep drawing tooling, plastic moulding dies, tools and plungers, die-casting plunger tips, non-magnetic and non sparking tools, electrical and electronic connectors, springs, fasteners, switchgear, resistance welding electrodes and equipment, flash butt welding dies and inserts, seam welding electrode shafts,Typical applications include bushings and bearings for aircraft as well as drill collars and instrument housings for oil and gas exploration.,EtchMet alloy is a material that is tailor made for the springs in voice coil motors and optical image stabilization systems common in smart phone cameras. | |
Corrosion properties | High corrosion resistance | |
General machinability | Very good machinability |