Allgemein
Property | Value | Condition |
---|---|---|
Dichte | 3.0 g/cm³ Show Material materials with Dichte of 3.0 g/cm³ | T7 |
Mechanisch
Property | Value | Condition | Comment |
---|---|---|---|
Dehnung | 12.0 % Show Material materials with Dehnung of 12.0 % | T7 | |
Elastizitätsmodul | 70.0 GPa Show Material materials with Elastizitätsmodul of 70.0 GPa | T7 | |
71 GPa Show Material materials with Elastizitätsmodul of 71 GPa | T7 | ||
Härte, Brinell | 130 [-] Show Material materials with Härte, Brinell of 130 [-] | T7 | 500 kg load, 10 mm b |
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | T7 | |
Scherfestigkeit | 260 MPa Show Material materials with Scherfestigkeit of 260 MPa | T7 | |
Schubmodule | 23.0 GPa Show Material materials with Schubmodule of 23.0 GPa | T7 | |
Streckgrenze | 350.0 MPa Show Material materials with Streckgrenze of 350.0 MPa | T7 | |
Zugfestigkeit | 440.0 MPa Show Material materials with Zugfestigkeit of 440.0 MPa | T7 |
Thermisch
Property | Value | Condition |
---|---|---|
Koeffizient der thermischen Ausdehnung | 2.1e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.1e-05 1/K | T7 |
Schmelzpunkt | 570.0 °C Show Material materials with Schmelzpunkt of 570.0 °C | T7 |
Spezifische Wärmekapazität | 920.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 920.0 J/(kg·K) | T7 |
Wärmeleitfähigkeit | 120.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 120.0 W/(m·K) | T7 |
Elektrisch
Property | Value | Condition | Comment |
---|---|---|---|
Elektrische Leitfähigkeit | 16000000.0 - 23000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 16000000.0 - 23000000.0 S/m | Typical for Cast 2xx.x Series Aluminium | |
spezifischer Widerstand | 5e-08 - 5.4e-08 Ω·m Show Material materials with spezifischer Widerstand of 5e-08 - 5.4e-08 Ω·m | T7 | Typical values |
Chemical properties
Property | Value | Condition |
---|---|---|
Aluminium | 93.3 - 95.3 % Show Material materials with Aluminium of 93.3 - 95.3 % | T7 |
Andere | 0.15 % Show Material materials with Andere of 0.15 % | T7 |
Eisen | 0.15 % Show Material materials with Eisen of 0.15 % | T7 |
Kupfer | 4.2 - 5.0 % Show Material materials with Kupfer of 4.2 - 5.0 % | T7 |
Magnesium | 0.15 - 0.35 % Show Material materials with Magnesium of 0.15 - 0.35 % | T7 |
Mangan | 0.2 - 0.5 % Show Material materials with Mangan of 0.2 - 0.5 % | T7 |
Nickel | 0.05 % Show Material materials with Nickel of 0.05 % | T7 |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % | T7 |
Titan | 0.15 - 0.3 % Show Material materials with Titan of 0.15 - 0.3 % | T7 |
Zink | 0.1 % Show Material materials with Zink of 0.1 % | T7 |
Zinn | 0.05 % Show Material materials with Zinn of 0.05 % | T7 |