Allgemein
Property | Value | Condition |
---|---|---|
Dichte | 4.5 g/cm³ Show Material materials with Dichte of 4.5 g/cm³ | Transformed-Beta |
Mechanisch
Property | Value | Condition |
---|---|---|
Dehnung | 6.9 % Show Material materials with Dehnung of 6.9 % | Transformed-Beta |
Elastizitätsmodul | 110.0 GPa Show Material materials with Elastizitätsmodul of 110.0 GPa | Transformed-Beta |
Streckgrenze | 870.0 MPa Show Material materials with Streckgrenze of 870.0 MPa | Transformed-Beta |
Zugfestigkeit | 950.0 MPa Show Material materials with Zugfestigkeit of 950.0 MPa | Transformed-Beta |
Thermisch
Property | Value | Condition | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 9.5e-06 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 9.5e-06 1/K | Transformed-Beta | |
Schmelzpunkt | 1500.0 - 1750.0 °C Show Material materials with Schmelzpunkt of 1500.0 - 1750.0 °C | Typical for Titanium Alpha Beta Alloy | |
Spezifische Wärmekapazität | 570.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 570.0 J/(kg·K) | Transformed-Beta | |
Wärmeleitfähigkeit | 7.3 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 7.3 W/(m·K) | Transformed-Beta |
Chemical properties
Property | Value | Condition |
---|---|---|
Aluminium | 5.5 - 6.5 % Show Material materials with Aluminium of 5.5 - 6.5 % | Transformed-Beta |
Andere | 0.4 % Show Material materials with Andere of 0.4 % | Transformed-Beta |
Eisen | 0.25 % Show Material materials with Eisen of 0.25 % | Transformed-Beta |
Kohlenstoff | 0.08 % Show Material materials with Kohlenstoff of 0.08 % | Transformed-Beta |
Ruthenium | 0.08 - 0.14 % Show Material materials with Ruthenium of 0.08 - 0.14 % | Transformed-Beta |
Sauerstoff | 0.13 % Show Material materials with Sauerstoff of 0.13 % | Transformed-Beta |
Stickstoff | 0.03 % Show Material materials with Stickstoff of 0.03 % | Transformed-Beta |
Titan | 88.0 - 90.9 % Show Material materials with Titan of 88.0 - 90.9 % | Transformed-Beta |
Vanadium | 3.5 - 4.5 % Show Material materials with Vanadium of 3.5 - 4.5 % | Transformed-Beta |
Wasserstoff | 0.015 % Show Material materials with Wasserstoff of 0.015 % | Transformed-Beta |