Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 2.1 g/cm³ Show Material materials with Dichte of 2.1 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 4.9 - 5.2 % Show Material materials with Dehnung of 4.9 - 5.2 % | |
Elastizitätsmodul | 23.0 °C | 44 GPa Show Material materials with Elastizitätsmodul of 44 GPa | |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Magnesium |
Schubmodule | 23.0 °C | 45 GPa Show Material materials with Schubmodule of 45 GPa | Typical for Magnesium |
Streckgrenze | 23.0 °C | 160 - 170 MPa Show Material materials with Streckgrenze of 160 - 170 MPa | |
Zugfestigkeit | 23.0 °C | 250 - 270 MPa Show Material materials with Zugfestigkeit of 250 - 270 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.7E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.7E-5 1/K |
Schmelzpunkt | 570 °C Show Material materials with Schmelzpunkt of 570 °C | |
Spezifische Wärmekapazität | 23.0 °C | 970 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 970 J/(kg·K) |
Wärmeleitfähigkeit | 23.0 °C | 26 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 26 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Andere | 0 - 0.3 % Show Material materials with Andere of 0 - 0.3 % |
Eisen | 0 - 0.01 % Show Material materials with Eisen of 0 - 0.01 % |
Kupfer | 0 - 0.03 % Show Material materials with Kupfer of 0 - 0.03 % |
Lithium | 0 - 0.2 % Show Material materials with Lithium of 0 - 0.2 % |
Magnesium | 89.5 - 93.5 % Show Material materials with Magnesium of 89.5 - 93.5 % |
Mangan | 0 - 0.15 % Show Material materials with Mangan of 0 - 0.15 % |
Nickel | 0 - 5E-3 % Show Material materials with Nickel of 0 - 5E-3 % |
Seltene-Erden-Elemente | 2.4 - 4.4 % Show Material materials with Seltene-Erden-Elemente of 2.4 - 4.4 % |
Silizium | 0 - 0.01 % Show Material materials with Silizium of 0 - 0.01 % |
Yttrium | 3.7 - 4.3 % Show Material materials with Yttrium of 3.7 - 4.3 % |
Zink | 0 - 0.2 % Show Material materials with Zink of 0 - 0.2 % |
Zirkonium | 0.4 - 1 % Show Material materials with Zirkonium of 0.4 - 1 % |