Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 9.9 g/cm³ Show Material materials with Dichte of 9.9 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 48 % Show Material materials with Dehnung of 48 % |
Elastizitätsmodul | 23.0 °C | 210 GPa Show Material materials with Elastizitätsmodul of 210 GPa |
Streckgrenze | 23.0 °C | 400 MPa Show Material materials with Streckgrenze of 400 MPa |
Zugfestigkeit | 23.0 °C | 840 MPa Show Material materials with Zugfestigkeit of 840 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.2E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.2E-5 1/K |
Schmelzpunkt | 1300 °C Show Material materials with Schmelzpunkt of 1300 °C | |
Spezifische Wärmekapazität | 23.0 °C | 400 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 400 J/(kg·K) |
Wärmeleitfähigkeit | 23.0 °C | 9 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 9 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.2 - 0.5 % Show Material materials with Aluminium of 0.2 - 0.5 % |
Bor | 0 - 0.015 % Show Material materials with Bor of 0 - 0.015 % |
Chrom | 20 - 24 % Show Material materials with Chrom of 20 - 24 % |
Eisen | 0 - 3 % Show Material materials with Eisen of 0 - 3 % |
Kobalt | 0 - 5 % Show Material materials with Kobalt of 0 - 5 % |
Kohlenstoff | 0.05 - 0.15 % Show Material materials with Kohlenstoff of 0.05 - 0.15 % |
Lanthan | 0.01 - 0.05 % Show Material materials with Lanthan of 0.01 - 0.05 % |
Mangan | 0.3 - 1 % Show Material materials with Mangan of 0.3 - 1 % |
Molybdän | 1 - 3 % Show Material materials with Molybdän of 1 - 3 % |
Nickel | 47.5 - 65.2 % Show Material materials with Nickel of 47.5 - 65.2 % |
Phosphor | 0 - 0.03 % Show Material materials with Phosphor of 0 - 0.03 % |
Schwefel | 0 - 0.015 % Show Material materials with Schwefel of 0 - 0.015 % |
Silizium | 0.25 - 0.75 % Show Material materials with Silizium of 0.25 - 0.75 % |
Wolfram | 13 - 15 % Show Material materials with Wolfram of 13 - 15 % |