Allgemein
Property | Value | Condition |
---|---|---|
Dichte | 3.1 g/cm³ Show Material materials with Dichte of 3.1 g/cm³ | T61 |
Mechanisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Dauerfestigkeit | 65 MPa Show Material materials with Dauerfestigkeit of 65 MPa | T61 | for 5x10⁸ cycles, R.R. Moore type test | ||
Dehnung | 0.5 % Show Material materials with Dehnung of 0.5 % | T61 | |||
0.5 % Show Material materials with Dehnung of 0.5 % | T61 | Sand cast, elongation in 50 mm | |||
Elastizitätsmodul | 71.0 GPa Show Material materials with Elastizitätsmodul of 71.0 GPa | T61 | |||
71 GPa Show Material materials with Elastizitätsmodul of 71 GPa | T61 | ||||
Härte, Brinell | 105.0 [-] Show Material materials with Härte, Brinell of 105.0 [-] | T61 | Pink Sheets, ASTM B26, ASTM B618 | Casting | |
110 [-] Show Material materials with Härte, Brinell of 110 [-] | T61 | 500 kg load, 10 mm b | |||
110.0 [-] Show Material materials with Härte, Brinell of 110.0 [-] | T61 | Pink Sheets, ASTM B108 | Casting | ||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | T61 | |||
Scherfestigkeit | 240 MPa Show Material materials with Scherfestigkeit of 240 MPa | T61 | |||
Schubmodule | 26.5 GPa Show Material materials with Schubmodule of 26.5 GPa | T61 | |||
Streckgrenze | 140.0 MPa Show Material materials with Streckgrenze of 140.0 MPa | T61 | Pink Sheets, ASTM B26, ASTM B618 | Casting | RP02 |
220.0 MPa Show Material materials with Streckgrenze of 220.0 MPa | T61 | ||||
290 MPa Show Material materials with Streckgrenze of 290 MPa | T61 | Sand cast, RP02 | |||
Zugfestigkeit | 220.0 MPa Show Material materials with Zugfestigkeit of 220.0 MPa | T61 | Pink Sheets, ASTM B26, ASTM B618 | Casting | |
240.0 MPa Show Material materials with Zugfestigkeit of 240.0 MPa | T61 | ||||
275.0 MPa Show Material materials with Zugfestigkeit of 275.0 MPa | T61 | Pink Sheets, ASTM B108 | Casting | ||
324 MPa Show Material materials with Zugfestigkeit of 324 MPa | T61 | Sand cast |
Thermisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 2.3e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.3e-05 1/K | T61 | ||||
100 °C | 0.0000225 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 0.0000225 1/K | T61 | nominal value between 20°C and the mentioned temperature | |||
300 °C | 0.0000245 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 0.0000245 1/K | T61 | nominal value between 20°C and the mentioned temperature | |||
Schmelzpunkt | 532.0 - 635.0 °C Show Material materials with Schmelzpunkt of 532.0 - 635.0 °C | T61 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting | ||
540.0 °C Show Material materials with Schmelzpunkt of 540.0 °C | T61 | |||||
Spezifische Wärmekapazität | 960.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 960.0 J/(kg·K) | T61 | ||||
Wärmeleitfähigkeit | 130.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 130.0 W/(m·K) | T61 | ||||
25 °C | 134 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 134 W/(m·K) | T61 | nominal value |
Elektrisch
Property | Value | Condition | Comment |
---|---|---|---|
Elektrische Leitfähigkeit | 19500000 S/m Show Material materials with Elektrische Leitfähigkeit of 19500000 S/m | T61 | Typical/Derived values |
Specific Electrical conductivity | 33.0 - 34.0 % IACS Show Material materials with Specific Electrical conductivity of 33.0 - 34.0 % IACS | T61 | Typical values |
spezifischer Widerstand | 5.2200000000000004e-08 Ω·m Show Material materials with spezifischer Widerstand of 5.2200000000000004e-08 Ω·m | T61 | Typical values |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminium | 88.4 - 93.6 % Show Material materials with Aluminium of 88.4 - 93.6 % | T61 | ||
Andere | 0.15 % Show Material materials with Andere of 0.15 % | T61 | ||
Chrom | 0.25 % Show Material materials with Chrom of 0.25 % | T61 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Eisen | 1.0 % Show Material materials with Eisen of 1.0 % | T61 | ||
1.00 % Show Material materials with Eisen of 1.00 % | T61 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting | |
Kupfer | 3.5 - 4.5 % Show Material materials with Kupfer of 3.5 - 4.5 % | T61 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Magnesium | 1.2 - 1.8 % Show Material materials with Magnesium of 1.2 - 1.8 % | T61 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Mangan | 0.35 % Show Material materials with Mangan of 0.35 % | T61 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Nickel | 1.7 - 2.3 % Show Material materials with Nickel of 1.7 - 2.3 % | T61 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Silizium | 0.7 % Show Material materials with Silizium of 0.7 % | T61 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Titan | 0.25 % Show Material materials with Titan of 0.25 % | T61 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Zink | 0.35 % Show Material materials with Zink of 0.35 % | T61 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |