Allgemein
Property | Value | Condition |
---|---|---|
Dichte | 3.1 g/cm³ Show Material materials with Dichte of 3.1 g/cm³ | T7 |
Mechanisch
Property | Value | Condition | Comment |
---|---|---|---|
Dehnung | 1.5 % Show Material materials with Dehnung of 1.5 % | T7 | |
Elastizitätsmodul | 71.0 GPa Show Material materials with Elastizitätsmodul of 71.0 GPa | T7 | |
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Cast 2xx.x Series Aluminium | |
Streckgrenze | 200.0 MPa Show Material materials with Streckgrenze of 200.0 MPa | T7 | |
Zugfestigkeit | 240.0 MPa Show Material materials with Zugfestigkeit of 240.0 MPa | T7 |
Thermisch
Property | Value | Condition |
---|---|---|
Koeffizient der thermischen Ausdehnung | 2.3e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.3e-05 1/K | T7 |
Schmelzpunkt | 540.0 °C Show Material materials with Schmelzpunkt of 540.0 °C | T7 |
Spezifische Wärmekapazität | 960.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 960.0 J/(kg·K) | T7 |
Wärmeleitfähigkeit | 150.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 150.0 W/(m·K) | T7 |
Elektrisch
Property | Value | Comment |
---|---|---|
Elektrische Leitfähigkeit | 16000000.0 - 23000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 16000000.0 - 23000000.0 S/m | Typical for Cast 2xx.x Series Aluminium |
spezifischer Widerstand | 4.347826086956522e-08 - 6.25e-08 Ω·m Show Material materials with spezifischer Widerstand of 4.347826086956522e-08 - 6.25e-08 Ω·m | Typical for Cast 2xx.x Series Aluminium |
Chemical properties
Property | Value | Condition |
---|---|---|
Aluminium | 88.4 - 93.6 % Show Material materials with Aluminium of 88.4 - 93.6 % | T7 |
Andere | 0.15 % Show Material materials with Andere of 0.15 % | T7 |
Chrom | 0.25 % Show Material materials with Chrom of 0.25 % | T7 |
Eisen | 1.0 % Show Material materials with Eisen of 1.0 % | T7 |
Kupfer | 3.5 - 4.5 % Show Material materials with Kupfer of 3.5 - 4.5 % | T7 |
Magnesium | 1.2 - 1.8 % Show Material materials with Magnesium of 1.2 - 1.8 % | T7 |
Mangan | 0.35 % Show Material materials with Mangan of 0.35 % | T7 |
Nickel | 1.7 - 2.3 % Show Material materials with Nickel of 1.7 - 2.3 % | T7 |
Silizium | 0.7 % Show Material materials with Silizium of 0.7 % | T7 |
Titan | 0.25 % Show Material materials with Titan of 0.25 % | T7 |
Zink | 0.35 % Show Material materials with Zink of 0.35 % | T7 |