Allgemein
Property | Value | Condition | Related Standards |
---|---|---|---|
Dichte | 2.73 g/cm³ Show Material materials with Dichte of 2.73 g/cm³ | H24 | AA Standards, ASTM B209 |
2.8 g/cm³ Show Material materials with Dichte of 2.8 g/cm³ | H24 |
Abmessung
Property | Value | Condition | Shape |
---|---|---|---|
Dimensions | <p>Standard process capabilities:</p> <p>Width: 10-1400mm</p> <p>Thickness 0.050-3.18mm</p> | H24 | Coil |
Mechanisch
Property | Value | Condition | Shape | Related Standards | Comment |
---|---|---|---|---|---|
Dehnung | 0.5 % Show Material materials with Dehnung of 0.5 % | H24 | Coil | Min., A50 | |
1.0 % Show Material materials with Dehnung of 1.0 % | H24 | AA Standards, ASTM B209 | A50 | ||
2.0 % Show Material materials with Dehnung of 2.0 % | H24 | AA Standards, ASTM B209 | A50 | ||
2.9 % Show Material materials with Dehnung of 2.9 % | H24 | ||||
3.0 % Show Material materials with Dehnung of 3.0 % | H24 | AA Standards, ASTM B209 | A50 | ||
5.0 % Show Material materials with Dehnung of 5.0 % | H24 | AA Standards, ASTM B209 | A50 | ||
7.0 % Show Material materials with Dehnung of 7.0 % | H24 | AA Standards, ASTM B209 | A100 | ||
8.0 % Show Material materials with Dehnung of 8.0 % | H24 | AA Standards, ASTM B209 | A50 | ||
20.0 % Show Material materials with Dehnung of 20.0 % | H24 | Coil | Min., A50 | ||
Elastizitätsmodul | 69.0 GPa Show Material materials with Elastizitätsmodul of 69.0 GPa | H24 | AA Standards, ASTM B209 | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 3000 Series Aluminium | |||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 3000 Series Aluminium | |||
Schubmodule | 25.0 - 26.0 GPa Show Material materials with Schubmodule of 25.0 - 26.0 GPa | Typical for Wrought 3000 Series Aluminium | |||
Streckgrenze | 50.0 MPa Show Material materials with Streckgrenze of 50.0 MPa | H24 | Coil | RP02 | |
115.0 MPa Show Material materials with Streckgrenze of 115.0 MPa | H24 | AA Standards, ASTM B209 | RP02 | ||
130.0 MPa Show Material materials with Streckgrenze of 130.0 MPa | H24 | ||||
160.0 MPa Show Material materials with Streckgrenze of 160.0 MPa | H24 | Coil | RP02 | ||
Zugfestigkeit | 110 MPa Show Material materials with Zugfestigkeit of 110 MPa | H24 | Coil | ||
140.0 - 180.0 MPa Show Material materials with Zugfestigkeit of 140.0 - 180.0 MPa | H24 | AA Standards, ASTM B209 | |||
160.0 - 220.0 MPa Show Material materials with Zugfestigkeit of 160.0 - 220.0 MPa | H24 | Coil | |||
160 MPa Show Material materials with Zugfestigkeit of 160 MPa | H24 |
Thermisch
Property | Temperature | Value | Condition | Shape | Related Standards | Comment |
---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 2.3e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.3e-05 1/K | H24 | ||||
2.36e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.36e-05 1/K | H24 | Coil | for 20-100°C | |||
20 °C | 2.3199999999999998e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.3199999999999998e-05 1/K | H24 | AA Standards, ASTM B209 | |||
100 °C | 2.3199999999999998e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.3199999999999998e-05 1/K | H24 | AA Standards, ASTM B209 | |||
Schmelzpunkt | 605 °C Show Material materials with Schmelzpunkt of 605 °C | H24 | Coil | Mean | ||
607 °C Show Material materials with Schmelzpunkt of 607 °C | H24 | Coil | Mean | |||
618 °C Show Material materials with Schmelzpunkt of 618 °C | H24 | Coil | Mean | |||
623 °C Show Material materials with Schmelzpunkt of 623 °C | H24 | Coil | Mean | |||
640 °C Show Material materials with Schmelzpunkt of 640 °C | H24 | Coil | Mean | |||
640.0 °C Show Material materials with Schmelzpunkt of 640.0 °C | H24 | |||||
640.0 - 655.0 °C Show Material materials with Schmelzpunkt of 640.0 - 655.0 °C | H24 | AA Standards, ASTM B209 | ||||
642 °C Show Material materials with Schmelzpunkt of 642 °C | H24 | Coil | Mean | |||
Spezifische Wärmekapazität | 889.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 889.0 J/(kg·K) | H24 | Coil | |||
890.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 890.0 J/(kg·K) | H24 | |||||
Wärmeleitfähigkeit | 159.0 - 193.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 159.0 - 193.0 W/(m·K) | H24 | AA Standards, ASTM B209 | |||
160 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 160 W/(m·K) | H24 | Coil | After brazing, calculated from electric resistivity data measured at room temperature | |||
180.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 180.0 W/(m·K) | H24 |
Elektrisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Elektrische Leitfähigkeit | 24000000.0 - 29000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 24000000.0 - 29000000.0 S/m | H24 | AA Standards, ASTM B209 | ||
Korrosionspotenzial | -720.0 mV Show Material materials with Korrosionspotenzial of -720.0 mV | H24 | Coil | ||
-705.0 mV Show Material materials with Korrosionspotenzial of -705.0 mV | H24 | Coil | |||
-690.0 mV Show Material materials with Korrosionspotenzial of -690.0 mV | H24 | Coil | |||
spezifischer Widerstand | 3.4e-08 - 4.3e-08 Ω·m Show Material materials with spezifischer Widerstand of 3.4e-08 - 4.3e-08 Ω·m | H24 | Coil | Changes depending on temper | |
3.45e-08 - 4.17e-08 Ω·m Show Material materials with spezifischer Widerstand of 3.45e-08 - 4.17e-08 Ω·m | H24 | AA Standards, ASTM B209 |
Chemical properties
Property | Value | Condition | Shape | Related Standards |
---|---|---|---|---|
Aluminium | 96.8 - 99.0 % Show Material materials with Aluminium of 96.8 - 99.0 % | H24 | ||
Andere | 0.15 % Show Material materials with Andere of 0.15 % | H24 | ||
Eisen | 0.1 - 0.5 % Show Material materials with Eisen of 0.1 - 0.5 % | H24 | Coil | |
0.7 % Show Material materials with Eisen of 0.7 % | H24 | |||
0.70 % Show Material materials with Eisen of 0.70 % | H24 | AA Standards, ASTM B209 | ||
Kupfer | 0.05 - 0.2 % Show Material materials with Kupfer of 0.05 - 0.2 % | H24 | AA Standards, ASTM B209 | |
0.4 - 0.7 % Show Material materials with Kupfer of 0.4 - 0.7 % | H24 | Coil | ||
Mangan | 1.0 - 1.5 % Show Material materials with Mangan of 1.0 - 1.5 % | H24 | AA Standards, ASTM B209 | |
1.2 - 1.6 % Show Material materials with Mangan of 1.2 - 1.6 % | H24 | Coil | ||
Silizium | 0.4 - 0.8 % Show Material materials with Silizium of 0.4 - 0.8 % | H24 | Coil | |
0.6 % Show Material materials with Silizium of 0.6 % | H24 | AA Standards, ASTM B209 | ||
Titan | 0.1 - 0.2 % Show Material materials with Titan of 0.1 - 0.2 % | H24 | Coil | |
Zink | 0.0 - 0.1 % Show Material materials with Zink of 0.0 - 0.1 % | H24 | Coil | |
0.05 % Show Material materials with Zink of 0.05 % | H24 | Coil | ||
0.10 % Show Material materials with Zink of 0.10 % | H24 | Coil | ||
0.1 % Show Material materials with Zink of 0.1 % | H24 | Coil | ||
0.1 % Show Material materials with Zink of 0.1 % | H24 | AA Standards, ASTM B209 | ||
0.2 % Show Material materials with Zink of 0.2 % | H24 | Coil | ||
Zirkonium | 0.0 - 0.1 % Show Material materials with Zirkonium of 0.0 - 0.1 % | H24 | Coil |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive, Heat Exchangers | |
Brazing | general: possible with commercial processes and methods | |
Corrosion properties | Stress corrosion cracking: no damage during operation and laboratory tests, general: very good, without protection in industrial or seawater atmosphere | |
General machinability | General: not suitable (O, H12), poor (H14, H16, H25) | |
Heat Treatment | Age Hardenable | |
Processing history | Temper: H24 | |
Workability | general (condition): good (O, H12), acceptable (H14, H25), poor(H16, H18) |