Allgemein
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Dichte | 2.73 g/cm³ Show Material materials with Dichte of 2.73 g/cm³ | H14 | BS EN 573-3, BS EN 485-2 | Sheet |
2.8 g/cm³ Show Material materials with Dichte of 2.8 g/cm³ | H14 |
Mechanisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Dehnung | 4.6 % Show Material materials with Dehnung of 4.6 % | H14 | |||
Elastizitätsmodul | 69.5 GPa Show Material materials with Elastizitätsmodul of 69.5 GPa | H14 | BS EN 573-3, BS EN 485-2 | Sheet | |
72.0 GPa Show Material materials with Elastizitätsmodul of 72.0 GPa | H14 | ||||
Härte, Brinell | 45.0 [-] Show Material materials with Härte, Brinell of 45.0 [-] | H14 | BS EN 573-3, BS EN 485-2 | Sheet | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 3000 Series Aluminium | |||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 3000 Series Aluminium | |||
Schubmodule | 25.0 - 26.0 GPa Show Material materials with Schubmodule of 25.0 - 26.0 GPa | Typical for Wrought 3000 Series Aluminium | |||
Streckgrenze | 130.0 MPa Show Material materials with Streckgrenze of 130.0 MPa | H14 | |||
Zugfestigkeit | 140.0 - 180.0 MPa Show Material materials with Zugfestigkeit of 140.0 - 180.0 MPa | H14 | BS EN 573-3, BS EN 485-2 | Sheet | |
150.0 MPa Show Material materials with Zugfestigkeit of 150.0 MPa | H14 |
Thermisch
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 2.3e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.3e-05 1/K | H14 | ||
2.31e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.31e-05 1/K | H14 | BS EN 573-3, BS EN 485-2 | Sheet | |
Schmelzpunkt | 640.0 °C Show Material materials with Schmelzpunkt of 640.0 °C | H14 | ||
655.0 °C Show Material materials with Schmelzpunkt of 655.0 °C | H14 | BS EN 573-3, BS EN 485-2 | Sheet | |
Spezifische Wärmekapazität | 890.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 890.0 J/(kg·K) | H14 | ||
Wärmeleitfähigkeit | 160.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 160.0 W/(m·K) | H14 | BS EN 573-3, BS EN 485-2 | Sheet |
Elektrisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Elektrische Leitfähigkeit | 23000000.0 - 29000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 23000000.0 - 29000000.0 S/m | Typical for Wrought 3000 Series Aluminium | |||
spezifischer Widerstand | 4.11e-08 Ω·m Show Material materials with spezifischer Widerstand of 4.11e-08 Ω·m | H14 | BS EN 573-3, BS EN 485-2 | Sheet |
Chemical properties
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Aluminium | 96.3 - 99.1 % Show Material materials with Aluminium of 96.3 - 99.1 % | H14 | |||
Andere | 0.15 % Show Material materials with Andere of 0.15 % | H14 | BS EN 573-3, BS EN 485-2 | Sheet | Total |
Chrom | 0.1 % Show Material materials with Chrom of 0.1 % | H14 | BS EN 573-3, BS EN 485-2 | Sheet | |
Eisen | 0.7 % Show Material materials with Eisen of 0.7 % | H14 | |||
Kupfer | 0.1 % Show Material materials with Kupfer of 0.1 % | H14 | BS EN 573-3, BS EN 485-2 | Sheet | |
Magnesium | 0.3 % Show Material materials with Magnesium of 0.3 % | H14 | BS EN 573-3, BS EN 485-2 | Sheet | |
Mangan | 0.9 - 1.5 % Show Material materials with Mangan of 0.9 - 1.5 % | H14 | BS EN 573-3, BS EN 485-2 | Sheet | |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % | H14 | BS EN 573-3, BS EN 485-2 | Sheet | |
Titan | 0.1 % Show Material materials with Titan of 0.1 % | H14 | BS EN 573-3, BS EN 485-2 | Sheet | Ti + Zr |
Zink | 0.2 % Show Material materials with Zink of 0.2 % | H14 | BS EN 573-3, BS EN 485-2 | Sheet | |
Zirkonium | 0.1 % Show Material materials with Zirkonium of 0.1 % | H14 |
Technological properties
Property | ||
---|---|---|
Brazing | Very Good | |
General machinability | Acceptable | |
Soldering general | Very Good | |
Welding | Gas: Very Good; Arc: Very Good; Resistance: Good | |
Workability | Cold: Good |