Allgemein
Property | Value | Condition |
---|---|---|
Dichte | 2.8 g/cm³ Show Material materials with Dichte of 2.8 g/cm³ | H18 |
Mechanisch
Property | Value | Condition | Comment |
---|---|---|---|
Dehnung | 2.3 % Show Material materials with Dehnung of 2.3 % | H18 | |
Elastizitätsmodul | 72.0 GPa Show Material materials with Elastizitätsmodul of 72.0 GPa | H18 | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 3000 Series Aluminium | |
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 3000 Series Aluminium | |
Schubmodule | 25.0 - 26.0 GPa Show Material materials with Schubmodule of 25.0 - 26.0 GPa | Typical for Wrought 3000 Series Aluminium | |
Streckgrenze | 180.0 MPa Show Material materials with Streckgrenze of 180.0 MPa | H18 | |
Zugfestigkeit | 210.0 MPa Show Material materials with Zugfestigkeit of 210.0 MPa | H18 |
Thermisch
Property | Temperature | Value | Condition | Comment |
---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 2.3e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.3e-05 1/K | H18 | ||
100 °C | 0.0000231 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 0.0000231 1/K | H18 | unstated value for 20-100°C | |
Schmelzpunkt | 640.0 °C Show Material materials with Schmelzpunkt of 640.0 °C | H18 | ||
Spezifische Wärmekapazität | 890.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 890.0 J/(kg·K) | H18 | ||
Wärmeleitfähigkeit | 160.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 160.0 W/(m·K) | H18 |
Elektrisch
Property | Value | Comment |
---|---|---|
Elektrische Leitfähigkeit | 23000000.0 - 29000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 23000000.0 - 29000000.0 S/m | Typical for Wrought 3000 Series Aluminium |
spezifischer Widerstand | 3.4e-08 - 4.2e-08 Ω·m Show Material materials with spezifischer Widerstand of 3.4e-08 - 4.2e-08 Ω·m | Typical for Wrought 3000 Series Aluminium |
Chemical properties
Property | Value | Condition |
---|---|---|
Aluminium | 96.3 - 99.1 % Show Material materials with Aluminium of 96.3 - 99.1 % | H18 |
Andere | 0.15 % Show Material materials with Andere of 0.15 % | H18 |
Chrom | 0.1 % Show Material materials with Chrom of 0.1 % | H18 |
Eisen | 0.7 % Show Material materials with Eisen of 0.7 % | H18 |
Kupfer | 0.1 % Show Material materials with Kupfer of 0.1 % | H18 |
Magnesium | 0.3 % Show Material materials with Magnesium of 0.3 % | H18 |
Mangan | 0.9 - 1.5 % Show Material materials with Mangan of 0.9 - 1.5 % | H18 |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % | H18 |
Titan | 0.1 % Show Material materials with Titan of 0.1 % | H18 |
Zink | 0.2 % Show Material materials with Zink of 0.2 % | H18 |
Zirkonium | 0.1 % Show Material materials with Zirkonium of 0.1 % | H18 |
Technological properties
Property | ||
---|---|---|
Workability | Good workability. |