Allgemein
Property | Value | Condition | Related Standards |
---|---|---|---|
Dichte | 2.72 g/cm³ Show Material materials with Dichte of 2.72 g/cm³ | H25 | AA Standards, ASTM B209 |
2.72 g/cm³ Show Material materials with Dichte of 2.72 g/cm³ | H25 | ||
2.8 g/cm³ Show Material materials with Dichte of 2.8 g/cm³ | H25 |
Mechanisch
Property | Value | Condition | Related Standards | Comment |
---|---|---|---|---|
Dehnung | 2.0 % Show Material materials with Dehnung of 2.0 % | H25 | AA Standards, ASTM B209 | A50 |
4.0 % Show Material materials with Dehnung of 4.0 % | H25 | AA Standards, ASTM B209 | A50 | |
6.0 % Show Material materials with Dehnung of 6.0 % | H25 | AA Standards, ASTM B209 | A50 | |
6.4 % Show Material materials with Dehnung of 6.4 % | H25 | |||
8 % Show Material materials with Dehnung of 8 % | H25 | |||
Elastizitätsmodul | 69.0 GPa Show Material materials with Elastizitätsmodul of 69.0 GPa | H25 | AA Standards, ASTM B209 | |
69 GPa Show Material materials with Elastizitätsmodul of 69 GPa | H25 | |||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 3000 Series Aluminium | ||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 3000 Series Aluminium | ||
Scherfestigkeit | 105.0 MPa Show Material materials with Scherfestigkeit of 105.0 MPa | H25 | ||
Schubmodule | 25.0 GPa Show Material materials with Schubmodule of 25.0 GPa | H25 | ||
Streckgrenze | 130.0 MPa Show Material materials with Streckgrenze of 130.0 MPa | H25 | AA Standards, ASTM B209 | RP02 |
160 MPa Show Material materials with Streckgrenze of 160 MPa | H25 | RP02 | ||
160.0 MPa Show Material materials with Streckgrenze of 160.0 MPa | H25 | |||
Zugfestigkeit | 160.0 MPa Show Material materials with Zugfestigkeit of 160.0 MPa | H25 | AA Standards, ASTM B209 | |
180.0 MPa Show Material materials with Zugfestigkeit of 180.0 MPa | H25 | |||
180 MPa Show Material materials with Zugfestigkeit of 180 MPa | H25 |
Thermisch
Property | Temperature | Value | Condition | Related Standards |
---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 2.4e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.4e-05 1/K | H25 | ||
20 °C | 2.36e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.36e-05 1/K | H25 | AA Standards, ASTM B209 | |
100 °C | 2.36e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.36e-05 1/K | H25 | AA Standards, ASTM B209 | |
Schmelzpunkt | 635.0 - 655.0 °C Show Material materials with Schmelzpunkt of 635.0 - 655.0 °C | H25 | AA Standards, ASTM B209 | |
640.0 °C Show Material materials with Schmelzpunkt of 640.0 °C | H25 | |||
Spezifische Wärmekapazität | 900.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 900.0 J/(kg·K) | H25 | ||
Wärmeleitfähigkeit | 170.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 170.0 W/(m·K) | H25 | ||
172 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 172 W/(m·K) | H25 | AA Standards, ASTM B209 |
Elektrisch
Property | Value | Condition | Related Standards |
---|---|---|---|
Elektrische Leitfähigkeit | 26000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 26000000.0 S/m | H25 | AA Standards, ASTM B209 |
spezifischer Widerstand | 3.85e-08 Ω·m Show Material materials with spezifischer Widerstand of 3.85e-08 Ω·m | H25 | AA Standards, ASTM B209 |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Aluminium | 96.0 - 99.5 % Show Material materials with Aluminium of 96.0 - 99.5 % | H25 | |
Andere | 0.15 % Show Material materials with Andere of 0.15 % | H25 | |
Chrom | 0.2 % Show Material materials with Chrom of 0.2 % | H25 | AA Standards, ASTM B209 |
Eisen | 0.70 % Show Material materials with Eisen of 0.70 % | H25 | AA Standards, ASTM B209 |
0.7 % Show Material materials with Eisen of 0.7 % | H25 | ||
Kupfer | 0.3 % Show Material materials with Kupfer of 0.3 % | H25 | AA Standards, ASTM B209 |
Magnesium | 0.2 - 0.8 % Show Material materials with Magnesium of 0.2 - 0.8 % | H25 | AA Standards, ASTM B209 |
Mangan | 0.3 - 0.8 % Show Material materials with Mangan of 0.3 - 0.8 % | H25 | AA Standards, ASTM B209 |
Silizium | 0.6 % Show Material materials with Silizium of 0.6 % | H25 | AA Standards, ASTM B209 |
Titan | 0.1 % Show Material materials with Titan of 0.1 % | H25 | AA Standards, ASTM B209 |
Zink | 0.4 % Show Material materials with Zink of 0.4 % | H25 | AA Standards, ASTM B209 |
Technological properties
Property | ||
---|---|---|
Brazing | general: possible with commercial processes and methods | |
Corrosion properties | Stress corrosion cracking: no damage during operation and laboratory tests, general: very good, without protection in industrial or seawater atmosphere | |
General machinability | General: not suitable (O, H12), poor (H14, H25, H16, H18) | |
Workability | general (condition): good (O), acceptable (H12, H14, H25), poor(H16, H18) |