Allgemein
Property | Value | Condition |
---|---|---|
Dichte | 3.0 g/cm³ Show Material materials with Dichte of 3.0 g/cm³ | T6 |
Mechanisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Compressive yield strength | 172.0 - 193.0 MPa Show Material materials with Compressive yield strength of 172.0 - 193.0 MPa | T6 | |||
Dauerfestigkeit | 76.0 - 83.0 MPa Show Material materials with Dauerfestigkeit of 76.0 - 83.0 MPa | T6 | for 5x10⁸ cycles, R.R. Moore type test | ||
Dehnung | 1.5 - 2.0 % Show Material materials with Dehnung of 1.5 - 2.0 % | T6 | Sand cast, elongation in 50 mm | ||
1.5 % Show Material materials with Dehnung of 1.5 % | T6 | Pink Sheets, ASTM B26, ASTM B618 | Casting | A100 | |
1.8 % Show Material materials with Dehnung of 1.8 % | T6 | ||||
Elastizitätsmodul | 74 GPa Show Material materials with Elastizitätsmodul of 74 GPa | T6 | |||
78.0 GPa Show Material materials with Elastizitätsmodul of 78.0 GPa | T6 | ||||
Härte, Brinell | 80.0 - 95.0 [-] Show Material materials with Härte, Brinell of 80.0 - 95.0 [-] | T6 | 500 kg load, 10 mm b | ||
80.0 [-] Show Material materials with Härte, Brinell of 80.0 [-] | T6 | Pink Sheets, ASTM B26, ASTM B618 | Casting | ||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | T6 | |||
Scherfestigkeit | 200.0 - 220.0 MPa Show Material materials with Scherfestigkeit of 200.0 - 220.0 MPa | T6 | |||
Schubmodule | 28.0 GPa Show Material materials with Schubmodule of 28.0 GPa | T6 | |||
Streckgrenze | 140.0 MPa Show Material materials with Streckgrenze of 140.0 MPa | T6 | Pink Sheets, ASTM B26, ASTM B618 | Casting | RP02 |
160.0 MPa Show Material materials with Streckgrenze of 160.0 MPa | T6 | ||||
164 MPa Show Material materials with Streckgrenze of 164 MPa | T6 | Sand cast, RP02 | |||
Zugfestigkeit | 215.0 MPa Show Material materials with Zugfestigkeit of 215.0 MPa | T6 | Pink Sheets, ASTM B26, ASTM B618 | Casting | |
250.0 MPa Show Material materials with Zugfestigkeit of 250.0 MPa | T6 | ||||
250 MPa Show Material materials with Zugfestigkeit of 250 MPa | T6 | Sand cast |
Thermisch
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 2.3e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.3e-05 1/K | T6 | ||
Schmelzpunkt | 510.0 - 607.0 °C Show Material materials with Schmelzpunkt of 510.0 - 607.0 °C | T6 | Pink Sheets, ASTM B26, ASTM B618 | Casting |
540.0 °C Show Material materials with Schmelzpunkt of 540.0 °C | T6 | |||
Spezifische Wärmekapazität | 860.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 860.0 J/(kg·K) | T6 | ||
Wärmeleitfähigkeit | 110.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 110.0 W/(m·K) | T6 |
Elektrisch
Property | Value | Condition | Comment |
---|---|---|---|
spezifischer Widerstand | 6.39e-08 Ω·m Show Material materials with spezifischer Widerstand of 6.39e-08 Ω·m | T6 | Typical values |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminium | 85.8 - 91.5 % Show Material materials with Aluminium of 85.8 - 91.5 % | T6 | ||
Andere | 0.5 % Show Material materials with Andere of 0.5 % | T6 | ||
Eisen | 1.0 % Show Material materials with Eisen of 1.0 % | T6 | ||
1.00 % Show Material materials with Eisen of 1.00 % | T6 | Pink Sheets, ASTM B26, ASTM B618 | Casting | |
Kupfer | 3.0 - 4.0 % Show Material materials with Kupfer of 3.0 - 4.0 % | T6 | Pink Sheets, ASTM B26, ASTM B618 | Casting |
Magnesium | 0.1 % Show Material materials with Magnesium of 0.1 % | T6 | Pink Sheets, ASTM B26, ASTM B618 | Casting |
Mangan | 0.5 % Show Material materials with Mangan of 0.5 % | T6 | Pink Sheets, ASTM B26, ASTM B618 | Casting |
Nickel | 0.35 % Show Material materials with Nickel of 0.35 % | T6 | Pink Sheets, ASTM B26, ASTM B618 | Casting |
Silizium | 5.5 - 6.5 % Show Material materials with Silizium of 5.5 - 6.5 % | T6 | Pink Sheets, ASTM B26, ASTM B618 | Casting |
Titan | 0.25 % Show Material materials with Titan of 0.25 % | T6 | Pink Sheets, ASTM B26, ASTM B618 | Casting |
Zink | 1.0 % Show Material materials with Zink of 1.0 % | T6 | Pink Sheets, ASTM B26, ASTM B618 | Casting |