Allgemein
Property | Value | Condition |
---|---|---|
Dichte | 2.7 g/cm³ Show Material materials with Dichte of 2.7 g/cm³ | F |
Mechanisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Dehnung | 2.0 % Show Material materials with Dehnung of 2.0 % | F | Pink Sheets, ASTM B26, ASTM B618 | Casting | A100 |
3.0 % Show Material materials with Dehnung of 3.0 % | F | Pink Sheets, ASTM B108 | Casting | A100 | |
3.8 % Show Material materials with Dehnung of 3.8 % | F | ||||
6 % Show Material materials with Dehnung of 6 % | F | Sand cast, elongation in 50 mm | |||
Elastizitätsmodul | 72.0 GPa Show Material materials with Elastizitätsmodul of 72.0 GPa | F | |||
72.4 GPa Show Material materials with Elastizitätsmodul of 72.4 GPa | F | ||||
Härte, Brinell | 55.0 [-] Show Material materials with Härte, Brinell of 55.0 [-] | F | Pink Sheets, ASTM B26, ASTM B618 | Casting | |
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | F | |||
Schubmodule | 27.2 GPa Show Material materials with Schubmodule of 27.2 GPa | F | |||
Streckgrenze | 65.0 MPa Show Material materials with Streckgrenze of 65.0 MPa | F | Pink Sheets, ASTM B26 | Casting | RP02 |
70.0 MPa Show Material materials with Streckgrenze of 70.0 MPa | F | Pink Sheets, ASTM B108 | Casting | RP02 | |
100.0 MPa Show Material materials with Streckgrenze of 100.0 MPa | F | ||||
124 MPa Show Material materials with Streckgrenze of 124 MPa | F | Sand cast, RP02 | |||
Zugfestigkeit | 130.0 MPa Show Material materials with Zugfestigkeit of 130.0 MPa | F | Pink Sheets, ASTM B26, ASTM B618 | Casting | |
145.0 MPa Show Material materials with Zugfestigkeit of 145.0 MPa | F | Pink Sheets, ASTM B108 | Casting | ||
164 MPa Show Material materials with Zugfestigkeit of 164 MPa | F | Sand cast |
Thermisch
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 2.2e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.2e-05 1/K | F | ||
Schmelzpunkt | 557.0 - 613.0 °C Show Material materials with Schmelzpunkt of 557.0 - 613.0 °C | F | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
570.0 °C Show Material materials with Schmelzpunkt of 570.0 °C | F | |||
Spezifische Wärmekapazität | 970.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 970.0 J/(kg·K) | F | ||
Wärmeleitfähigkeit | 160.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 160.0 W/(m·K) | F |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminium | 90.1 - 93.3 % Show Material materials with Aluminium of 90.1 - 93.3 % | F | ||
Andere | 0.15 % Show Material materials with Andere of 0.15 % | F | ||
Eisen | 0.6 % Show Material materials with Eisen of 0.6 % | F | ||
0.60 % Show Material materials with Eisen of 0.60 % | F | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting | |
Kupfer | 0.25 % Show Material materials with Kupfer of 0.25 % | F | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Magnesium | 0.2 - 0.45 % Show Material materials with Magnesium of 0.2 - 0.45 % | F | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Mangan | 0.35 % Show Material materials with Mangan of 0.35 % | F | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Silizium | 6.5 - 7.5 % Show Material materials with Silizium of 6.5 - 7.5 % | F | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Titan | 0.25 % Show Material materials with Titan of 0.25 % | F | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Zink | 0.35 % Show Material materials with Zink of 0.35 % | F | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |