Allgemein
Property | Value | Condition |
---|---|---|
Dichte | 2.7 g/cm³ Show Material materials with Dichte of 2.7 g/cm³ | T5 |
Mechanisch
Property | Value | Condition | Comment |
---|---|---|---|
Dehnung | 2.0 % Show Material materials with Dehnung of 2.0 % | T5 | |
Elastizitätsmodul | 72.0 GPa Show Material materials with Elastizitätsmodul of 72.0 GPa | T5 | |
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Cast 3xx.x Series Aluminium | |
Schubmodule | 2.8 GPa Show Material materials with Schubmodule of 2.8 GPa | Typical for Cast 3xx.x Series Aluminium | |
Streckgrenze | 140.0 MPa Show Material materials with Streckgrenze of 140.0 MPa | T5 | |
Zugfestigkeit | 170.0 MPa Show Material materials with Zugfestigkeit of 170.0 MPa | T5 |
Thermisch
Property | Value | Condition |
---|---|---|
Koeffizient der thermischen Ausdehnung | 2.2e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.2e-05 1/K | T5 |
Schmelzpunkt | 570.0 °C Show Material materials with Schmelzpunkt of 570.0 °C | T5 |
Spezifische Wärmekapazität | 970.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 970.0 J/(kg·K) | T5 |
Wärmeleitfähigkeit | 170.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 170.0 W/(m·K) | T5 |
Chemical properties
Property | Value | Condition |
---|---|---|
Aluminium | 90.1 - 93.3 % Show Material materials with Aluminium of 90.1 - 93.3 % | T5 |
Andere | 0.15 % Show Material materials with Andere of 0.15 % | T5 |
Eisen | 0.6 % Show Material materials with Eisen of 0.6 % | T5 |
Kupfer | 0.25 % Show Material materials with Kupfer of 0.25 % | T5 |
Magnesium | 0.2 - 0.45 % Show Material materials with Magnesium of 0.2 - 0.45 % | T5 |
Mangan | 0.35 % Show Material materials with Mangan of 0.35 % | T5 |
Silizium | 6.5 - 7.5 % Show Material materials with Silizium of 6.5 - 7.5 % | T5 |
Titan | 0.25 % Show Material materials with Titan of 0.25 % | T5 |
Zink | 0.35 % Show Material materials with Zink of 0.35 % | T5 |