Allgemein
Property | Value | Condition |
---|---|---|
Dichte | 2.7 g/cm³ Show Material materials with Dichte of 2.7 g/cm³ | H15 |
Mechanisch
Property | Value | Condition | Comment |
---|---|---|---|
Dehnung | 3.5 % Show Material materials with Dehnung of 3.5 % | H15 | |
Elastizitätsmodul | 71.0 GPa Show Material materials with Elastizitätsmodul of 71.0 GPa | H15 | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 5000 Series Aluminium | |
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 5000 Series Aluminium | |
Schubmodule | 26.0 - 26.5 GPa Show Material materials with Schubmodule of 26.0 - 26.5 GPa | Typical for Wrought 5000 Series Aluminium | |
Streckgrenze | 210.0 MPa Show Material materials with Streckgrenze of 210.0 MPa | H15 | |
Zugfestigkeit | 270.0 MPa Show Material materials with Zugfestigkeit of 270.0 MPa | H15 |
Thermisch
Property | Value | Condition | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 2.4e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.4e-05 1/K | H15 | |
Max. Betriebstemperatur | 150.0 °C Show Material materials with Max. Betriebstemperatur of 150.0 °C | Typical for Wrought 5000 Series Aluminium | |
Schmelzpunkt | 620.0 °C Show Material materials with Schmelzpunkt of 620.0 °C | H15 | |
Spezifische Wärmekapazität | 900.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 900.0 J/(kg·K) | H15 | |
Wärmeleitfähigkeit | 140.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 140.0 W/(m·K) | H15 |
Elektrisch
Property | Value | Comment |
---|---|---|
Elektrische Leitfähigkeit | 18000000.0 - 31000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 18000000.0 - 31000000.0 S/m | Typical for Wrought 5000 Series Aluminium |
spezifischer Widerstand | 3.3e-08 - 5e-08 Ω·m Show Material materials with spezifischer Widerstand of 3.3e-08 - 5e-08 Ω·m | Typical for Wrought 5000 Series Aluminium |
Chemical properties
Property | Value | Condition |
---|---|---|
Aluminium | 94.7 - 97.9 % Show Material materials with Aluminium of 94.7 - 97.9 % | H15 |
Andere | 0.15 % Show Material materials with Andere of 0.15 % | H15 |
Chrom | 0.3 % Show Material materials with Chrom of 0.3 % | H15 |
Eisen | 0.5 % Show Material materials with Eisen of 0.5 % | H15 |
Kupfer | 0.1 % Show Material materials with Kupfer of 0.1 % | H15 |
Magnesium | 1.6 - 2.5 % Show Material materials with Magnesium of 1.6 - 2.5 % | H15 |
Mangan | 0.5 - 1.1 % Show Material materials with Mangan of 0.5 - 1.1 % | H15 |
Silizium | 0.4 % Show Material materials with Silizium of 0.4 % | H15 |
Titan | 0.1 % Show Material materials with Titan of 0.1 % | H15 |
Zink | 0.2 % Show Material materials with Zink of 0.2 % | H15 |
Technological properties
Property | ||
---|---|---|
Workability | Good workability. |