Allgemein
Property | Value | Condition |
---|---|---|
Dichte | 2.69 g/cm³ Show Material materials with Dichte of 2.69 g/cm³ | H38 |
2.7 g/cm³ Show Material materials with Dichte of 2.7 g/cm³ | H38 |
Mechanisch
Property | Value | Condition | Comment |
---|---|---|---|
Dehnung | 3.5 % Show Material materials with Dehnung of 3.5 % | H38 | |
Elastizitätsmodul | 71.0 GPa Show Material materials with Elastizitätsmodul of 71.0 GPa | H38 | |
Kompressionsmodul | 71.0 MPa Show Material materials with Kompressionsmodul of 71.0 MPa | H38 | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 5000 Series Aluminium | |
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 5000 Series Aluminium | |
Schubmodule | 26.0 - 26.5 GPa Show Material materials with Schubmodule of 26.0 - 26.5 GPa | Typical for Wrought 5000 Series Aluminium | |
Streckgrenze | 290.0 MPa Show Material materials with Streckgrenze of 290.0 MPa | H38 | |
Zugfestigkeit | 360.0 MPa Show Material materials with Zugfestigkeit of 360.0 MPa | H38 |
Thermisch
Property | Value | Condition | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 2.4e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.4e-05 1/K | H38 | |
Max. Betriebstemperatur | 150.0 °C Show Material materials with Max. Betriebstemperatur of 150.0 °C | Typical for Wrought 5000 Series Aluminium | |
Schmelzpunkt | 600.0 °C Show Material materials with Schmelzpunkt of 600.0 °C | H38 | |
Spezifische Wärmekapazität | 900.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 900.0 J/(kg·K) | H38 | |
Wärmeleitfähigkeit | 130.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 130.0 W/(m·K) | H38 |
Elektrisch
Property | Value | Condition | Comment |
---|---|---|---|
Elektrische Leitfähigkeit | 19700000 S/m Show Material materials with Elektrische Leitfähigkeit of 19700000 S/m | H38 | Typical/derived value |
Specific Electrical conductivity | 34.0 % IACS Show Material materials with Specific Electrical conductivity of 34.0 % IACS | H38 | Typical value |
spezifischer Widerstand | 3.3e-08 - 5e-08 Ω·m Show Material materials with spezifischer Widerstand of 3.3e-08 - 5e-08 Ω·m | Typical for Wrought 5000 Series Aluminium |
Chemical properties
Property | Value | Condition |
---|---|---|
Aluminium | 94.5 - 97.1 % Show Material materials with Aluminium of 94.5 - 97.1 % | H38 |
Andere | 0.15 % Show Material materials with Andere of 0.15 % | H38 |
Chrom | 0.05 - 0.2 % Show Material materials with Chrom of 0.05 - 0.2 % | H38 |
Eisen | 0.4 % Show Material materials with Eisen of 0.4 % | H38 |
Kupfer | 0.1 % Show Material materials with Kupfer of 0.1 % | H38 |
Magnesium | 2.4 - 3.0 % Show Material materials with Magnesium of 2.4 - 3.0 % | H38 |
Mangan | 0.5 - 1.0 % Show Material materials with Mangan of 0.5 - 1.0 % | H38 |
Silizium | 0.25 % Show Material materials with Silizium of 0.25 % | H38 |
Titan | 0.2 % Show Material materials with Titan of 0.2 % | H38 |
Zink | 0.25 % Show Material materials with Zink of 0.25 % | H38 |
Technological properties
Property | ||
---|---|---|
Workability | Good workability. |