Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 2.7 g/cm³ Show Material materials with Dichte of 2.7 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 11 % Show Material materials with Dehnung of 11 % |
Dehnung A50 | 20.0 °C | 8 - 12 % Show Material materials with Dehnung A50 of 8 - 12 % |
Elastizitätsmodul | 20.0 °C | 69 GPa Show Material materials with Elastizitätsmodul of 69 GPa |
Härte, Brinell | 20.0 °C | 73 [-] Show Material materials with Härte, Brinell of 73 [-] |
Streckgrenze | 20.0 °C | 210 MPa Show Material materials with Streckgrenze of 210 MPa |
Streckgrenze Rp 0,2 | 20.0 °C | 170 - 215 MPa Show Material materials with Streckgrenze Rp 0,2 of 170 - 215 MPa |
Zugfestigkeit | 20.0 °C | 205 - 250 MPa Show Material materials with Zugfestigkeit of 205 - 250 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 20.0 °C | 2.3E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.3E-5 1/K |
Schmelzpunkt | 620 °C Show Material materials with Schmelzpunkt of 620 °C | |
Spezifische Wärmekapazität | 20.0 °C | 900 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 900 J/(kg·K) |
Wärmeleitfähigkeit | 20.0 °C | 200 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 200 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Aluminium | 97.5 - 99.4 % Show Material materials with Aluminium of 97.5 - 99.4 % |
Andere | 0.15 % Show Material materials with Andere of 0.15 % |
Chrom | 0.1 % Show Material materials with Chrom of 0.1 % |
Eisen | 0.35 % Show Material materials with Eisen of 0.35 % |
Kupfer | 0.1 % Show Material materials with Kupfer of 0.1 % |
Magnesium | 0.45 - 0.9 % Show Material materials with Magnesium of 0.45 - 0.9 % |
Mangan | 0.1 % Show Material materials with Mangan of 0.1 % |
Silizium | 0.2 - 0.6 % Show Material materials with Silizium of 0.2 - 0.6 % |
Titan | 0.1 % Show Material materials with Titan of 0.1 % |
Zink | 0.1 % Show Material materials with Zink of 0.1 % |