Allgemein
Property | Value | Condition |
---|---|---|
Dichte | 2.7 g/cm³ Show Material materials with Dichte of 2.7 g/cm³ | T66 |
Mechanisch
Property | Value | Condition | Comment |
---|---|---|---|
Dehnung | 12.0 % Show Material materials with Dehnung of 12.0 % | T66 | |
Elastizitätsmodul | 69.0 GPa Show Material materials with Elastizitätsmodul of 69.0 GPa | T66 | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 6000 Series Aluminium | |
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 6000 Series Aluminium | |
Schubmodule | 26.0 - 26.5 GPa Show Material materials with Schubmodule of 26.0 - 26.5 GPa | Typical for Wrought 6000 Series Aluminium | |
Streckgrenze | 230.0 MPa Show Material materials with Streckgrenze of 230.0 MPa | T66 | |
Zugfestigkeit | 260.0 MPa Show Material materials with Zugfestigkeit of 260.0 MPa | T66 |
Thermisch
Property | Value | Condition |
---|---|---|
Koeffizient der thermischen Ausdehnung | 2.3e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.3e-05 1/K | T66 |
Schmelzpunkt | 620.0 °C Show Material materials with Schmelzpunkt of 620.0 °C | T66 |
Spezifische Wärmekapazität | 900.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 900.0 J/(kg·K) | T66 |
Wärmeleitfähigkeit | 200.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 200.0 W/(m·K) | T66 |
Elektrisch
Property | Value | Comment |
---|---|---|
Elektrische Leitfähigkeit | 21000000.0 - 34000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 21000000.0 - 34000000.0 S/m | Typical for Wrought 6000 Series Aluminium |
spezifischer Widerstand | 2.9e-08 - 5e-08 Ω·m Show Material materials with spezifischer Widerstand of 2.9e-08 - 5e-08 Ω·m | Typical for Wrought 6000 Series Aluminium |
Chemical properties
Property | Value | Condition |
---|---|---|
Aluminium | 97.5 - 99.4 % Show Material materials with Aluminium of 97.5 - 99.4 % | T66 |
Andere | 0.15 % Show Material materials with Andere of 0.15 % | T66 |
Chrom | 0.1 % Show Material materials with Chrom of 0.1 % | T66 |
Eisen | 0.35 % Show Material materials with Eisen of 0.35 % | T66 |
Kupfer | 0.1 % Show Material materials with Kupfer of 0.1 % | T66 |
Magnesium | 0.45 - 0.9 % Show Material materials with Magnesium of 0.45 - 0.9 % | T66 |
Mangan | 0.1 % Show Material materials with Mangan of 0.1 % | T66 |
Silizium | 0.2 - 0.6 % Show Material materials with Silizium of 0.2 - 0.6 % | T66 |
Titan | 0.1 % Show Material materials with Titan of 0.1 % | T66 |
Zink | 0.1 % Show Material materials with Zink of 0.1 % | T66 |
Technological properties
Property | ||
---|---|---|
Workability | Excellent workability. |