Allgemein
Property | Value | Condition |
---|---|---|
Dichte | 2.9 g/cm³ Show Material materials with Dichte of 2.9 g/cm³ | T5 |
Mechanisch
Property | Value | Condition | Comment |
---|---|---|---|
Dehnung | 15.0 % Show Material materials with Dehnung of 15.0 % | T5 | |
Elastizitätsmodul | 71.0 GPa Show Material materials with Elastizitätsmodul of 71.0 GPa | T5 | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 7000 Series Aluminium | |
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 7000 Series Aluminium | |
Schubmodule | 26.4 - 27.1 GPa Show Material materials with Schubmodule of 26.4 - 27.1 GPa | Typical for Wrought 7000 Series Aluminium | |
Streckgrenze | 350.0 MPa Show Material materials with Streckgrenze of 350.0 MPa | T5 | |
Zugfestigkeit | 400.0 MPa Show Material materials with Zugfestigkeit of 400.0 MPa | T5 |
Thermisch
Property | Value | Condition |
---|---|---|
Koeffizient der thermischen Ausdehnung | 2.3e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.3e-05 1/K | T5 |
Schmelzpunkt | 610.0 °C Show Material materials with Schmelzpunkt of 610.0 °C | T5 |
Spezifische Wärmekapazität | 880.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 880.0 J/(kg·K) | T5 |
Wärmeleitfähigkeit | 150.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 150.0 W/(m·K) | T5 |
Elektrisch
Property | Value | Comment |
---|---|---|
Elektrische Leitfähigkeit | 18000000.0 - 34000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 18000000.0 - 34000000.0 S/m | Typical for Wrought 7000 Series Aluminium |
spezifischer Widerstand | 2.9e-08 - 5.6e-08 Ω·m Show Material materials with spezifischer Widerstand of 2.9e-08 - 5.6e-08 Ω·m | Typical for Wrought 7000 Series Aluminium |
Chemical properties
Property | Value | Condition |
---|---|---|
Aluminium | 91.0 - 94.7 % Show Material materials with Aluminium of 91.0 - 94.7 % | T5 |
Andere | 0.15 % Show Material materials with Andere of 0.15 % | T5 |
Chrom | 0.06 - 0.2 % Show Material materials with Chrom of 0.06 - 0.2 % | T5 |
Eisen | 0.4 % Show Material materials with Eisen of 0.4 % | T5 |
Kupfer | 0.1 % Show Material materials with Kupfer of 0.1 % | T5 |
Magnesium | 1.0 - 1.8 % Show Material materials with Magnesium of 1.0 - 1.8 % | T5 |
Mangan | 0.2 - 0.7 % Show Material materials with Mangan of 0.2 - 0.7 % | T5 |
Silizium | 0.35 % Show Material materials with Silizium of 0.35 % | T5 |
Titan | 0.01 - 0.06 % Show Material materials with Titan of 0.01 - 0.06 % | T5 |
Zink | 4.0 - 5.0 % Show Material materials with Zink of 4.0 - 5.0 % | T5 |
Zirkonium | 0.08 - 0.2 % Show Material materials with Zirkonium of 0.08 - 0.2 % | T5 |
Technological properties
Property | ||
---|---|---|
Brazing | Excellent |