Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 3.1 g/cm³ Show Material materials with Dichte of 3.1 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 5.5 % Show Material materials with Dehnung of 5.5 % |
Dehnung A50 | 20.0 °C | 5 - 9 % Show Material materials with Dehnung A50 of 5 - 9 % |
Elastizitätsmodul | 20.0 °C | 72 GPa Show Material materials with Elastizitätsmodul of 72 GPa |
Streckgrenze | 20.0 °C | 470 MPa Show Material materials with Streckgrenze of 470 MPa |
Streckgrenze Rp 0,2 | 20.0 °C | 370 - 505 MPa Show Material materials with Streckgrenze Rp 0,2 of 370 - 505 MPa |
Zugfestigkeit | 20.0 °C | 460 - 570 MPa Show Material materials with Zugfestigkeit of 460 - 570 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 20.0 °C | 2.3E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.3E-5 1/K |
Schmelzpunkt | 480 °C Show Material materials with Schmelzpunkt of 480 °C | |
Spezifische Wärmekapazität | 20.0 °C | 910 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 910 J/(kg·K) |
Wärmeleitfähigkeit | 20.0 °C | 130 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 130 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Aluminium | 86.9 - 91.4 % Show Material materials with Aluminium of 86.9 - 91.4 % |
Andere | 0.15 % Show Material materials with Andere of 0.15 % |
Chrom | 0.18 - 0.28 % Show Material materials with Chrom of 0.18 - 0.28 % |
Eisen | 0.5 % Show Material materials with Eisen of 0.5 % |
Kupfer | 1.2 - 2 % Show Material materials with Kupfer of 1.2 - 2 % |
Magnesium | 2.1 - 2.9 % Show Material materials with Magnesium of 2.1 - 2.9 % |
Mangan | 0.3 % Show Material materials with Mangan of 0.3 % |
Silizium | 0.4 % Show Material materials with Silizium of 0.4 % |
Titan | 0.2 % Show Material materials with Titan of 0.2 % |
Zink | 5.1 - 6.1 % Show Material materials with Zink of 5.1 - 6.1 % |
Zirkonium | 0.25 % Show Material materials with Zirkonium of 0.25 % |