Allgemein
Property | Value | Condition |
---|---|---|
Dichte | 4.5 g/cm³ Show Material materials with Dichte of 4.5 g/cm³ | Annealed |
Mechanisch
Property | Value | Condition |
---|---|---|
Dehnung | 17.0 % Show Material materials with Dehnung of 17.0 % | Annealed |
Elastizitätsmodul | 110.0 GPa Show Material materials with Elastizitätsmodul of 110.0 GPa | Annealed |
Streckgrenze | 560.0 MPa Show Material materials with Streckgrenze of 560.0 MPa | Annealed |
Zugfestigkeit | 710.0 MPa Show Material materials with Zugfestigkeit of 710.0 MPa | Annealed |
Thermisch
Property | Value | Condition | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 9.9e-06 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 9.9e-06 1/K | Annealed | |
Schmelzpunkt | 1540.0 - 1715.0 °C Show Material materials with Schmelzpunkt of 1540.0 - 1715.0 °C | Typical for Titanium Near Alpha Alloy | |
Spezifische Wärmekapazität | 540.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 540.0 J/(kg·K) | Annealed | |
Wärmeleitfähigkeit | 8.3 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 8.3 W/(m·K) | Annealed |
Chemical properties
Property | Value | Condition |
---|---|---|
Aluminium | 2.5 - 3.5 % Show Material materials with Aluminium of 2.5 - 3.5 % | Annealed |
Andere | 0.4 % Show Material materials with Andere of 0.4 % | Annealed |
Eisen | 0.25 % Show Material materials with Eisen of 0.25 % | Annealed |
Kohlenstoff | 0.08 % Show Material materials with Kohlenstoff of 0.08 % | Annealed |
Ruthenium | 0.08 - 0.14 % Show Material materials with Ruthenium of 0.08 - 0.14 % | Annealed |
Sauerstoff | 0.15 % Show Material materials with Sauerstoff of 0.15 % | Annealed |
Stickstoff | 0.03 % Show Material materials with Stickstoff of 0.03 % | Annealed |
Titan | 92.4 - 95.4 % Show Material materials with Titan of 92.4 - 95.4 % | Annealed |
Vanadium | 2.0 - 3.0 % Show Material materials with Vanadium of 2.0 - 3.0 % | Annealed |
Wasserstoff | 0.015 % Show Material materials with Wasserstoff of 0.015 % | Annealed |