Allgemein
Property | Value | Condition | Related Standards |
---|---|---|---|
Dichte | 4.42 g/cm³ Show Material materials with Dichte of 4.42 g/cm³ | Annealed | AMS 4928, ASTM B348, ASTM F136 |
Mechanisch
Property | Value | Condition | Related Standards |
---|---|---|---|
Elastizitätsmodul | 105.0 - 120.0 GPa Show Material materials with Elastizitätsmodul of 105.0 - 120.0 GPa | Annealed | AMS 4928, ASTM B348, ASTM F136 |
Zugfestigkeit | 950.0 - 1100.0 MPa Show Material materials with Zugfestigkeit of 950.0 - 1100.0 MPa | Annealed | AMS 4928, ASTM B348, ASTM F136 |
Thermisch
Property | Value | Condition | Related Standards |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 9e-06 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 9e-06 1/K | Annealed | AMS 4928, ASTM B348, ASTM F136 |
Schmelzpunkt | 1605.0 °C Show Material materials with Schmelzpunkt of 1605.0 °C | Annealed | AMS 4928, ASTM B348, ASTM F136 |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Aluminium | 5.5 - 6.75 % Show Material materials with Aluminium of 5.5 - 6.75 % | Annealed | AMS 4928, ASTM B348, ASTM F136 |
Eisen | 0.4 Show Material materials with Eisen of 0.4 | Annealed | AMS 4928, ASTM B348, ASTM F136 |
Kohlenstoff | 0.1 Show Material materials with Kohlenstoff of 0.1 | Annealed | AMS 4928, ASTM B348, ASTM F136 |
Sauerstoff | 0.2 Show Material materials with Sauerstoff of 0.2 | Annealed | AMS 4928, ASTM B348, ASTM F136 |
Stickstoff | 0.05 Show Material materials with Stickstoff of 0.05 | Annealed | AMS 4928, ASTM B348, ASTM F136 |
Vanadium | 3.5 - 4.5 % Show Material materials with Vanadium of 3.5 - 4.5 % | Annealed | AMS 4928, ASTM B348, ASTM F136 |
Technological properties
Property | ||
---|---|---|