Allgemein
Property | Value | Condition |
---|---|---|
Dichte | 4.5 g/cm³ Show Material materials with Dichte of 4.5 g/cm³ | Annealed |
Mechanisch
Property | Value | Condition | Shape |
---|---|---|---|
Dehnung | 17.0 % Show Material materials with Dehnung of 17.0 % | Annealed | |
Elastizitätsmodul | 110.0 GPa Show Material materials with Elastizitätsmodul of 110.0 GPa | Annealed | |
Streckgrenze | 483.0 MPa Show Material materials with Streckgrenze of 483.0 MPa | Annealed | Sheet, Welded tube, bar |
560.0 MPa Show Material materials with Streckgrenze of 560.0 MPa | Annealed | ||
Zugfestigkeit | 620.0 MPa Show Material materials with Zugfestigkeit of 620.0 MPa | Annealed | Sheet, Welded tube, bar |
710.0 MPa Show Material materials with Zugfestigkeit of 710.0 MPa | Annealed |
Thermisch
Property | Value | Condition | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 9.1e-06 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 9.1e-06 1/K | Annealed | |
Schmelzpunkt | 1668.0 °C Show Material materials with Schmelzpunkt of 1668.0 °C | Typical for Titanium | |
Spezifische Wärmekapazität | 490.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 490.0 J/(kg·K) | Annealed | |
Wärmeleitfähigkeit | 8.1 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 8.1 W/(m·K) | Annealed |
Chemical properties
Property | Value | Condition | Shape |
---|---|---|---|
Aluminium | 2.5 - 3.5 % Show Material materials with Aluminium of 2.5 - 3.5 % | Annealed | |
2.5 - 3.0 % Show Material materials with Aluminium of 2.5 - 3.0 % | Annealed | Sheet, Welded tube, bar | |
Andere | 0.4 % Show Material materials with Andere of 0.4 % | Annealed | |
Eisen | 0.25 % Show Material materials with Eisen of 0.25 % | Annealed | Sheet, Welded tube, bar |
Kohlenstoff | 0.08 % Show Material materials with Kohlenstoff of 0.08 % | Annealed | Sheet, Welded tube, bar |
Sauerstoff | 0.15 % Show Material materials with Sauerstoff of 0.15 % | Annealed | Sheet, Welded tube, bar |
Stickstoff | 0.03 % Show Material materials with Stickstoff of 0.03 % | Annealed | Sheet, Welded tube, bar |
Titan | 92.6 - 95.5 % Show Material materials with Titan of 92.6 - 95.5 % | Annealed | |
Vanadium | 2.0 - 3.0 % Show Material materials with Vanadium of 2.0 - 3.0 % | Annealed | Sheet, Welded tube, bar |
Wasserstoff | 0.015 % Show Material materials with Wasserstoff of 0.015 % | Annealed |