Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.4 g/cm³ Show Material materials with Dichte of 8.4 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 12 % Show Material materials with Dehnung of 12 % |
Elastizitätsmodul | 23.0 °C | 210 GPa Show Material materials with Elastizitätsmodul of 210 GPa |
Streckgrenze | 23.0 °C | 480 MPa Show Material materials with Streckgrenze of 480 MPa |
Zugfestigkeit | 23.0 °C | 780 MPa Show Material materials with Zugfestigkeit of 780 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.2E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.2E-5 1/K |
Spezifische Wärmekapazität | 23.0 °C | 450 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 450 J/(kg·K) |
Wärmeleitfähigkeit | 23.0 °C | 13 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 13 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Aluminium | 0 - 0.1 % Show Material materials with Aluminium of 0 - 0.1 % |
Bor | 0 - 0.01 % Show Material materials with Bor of 0 - 0.01 % |
Chrom | 27 - 30 % Show Material materials with Chrom of 27 - 30 % |
Eisen | 0 - 0.75 % Show Material materials with Eisen of 0 - 0.75 % |
Kobalt | 58.7 - 68 % Show Material materials with Kobalt of 58.7 - 68 % |
Kohlenstoff | 0 - 0.35 % Show Material materials with Kohlenstoff of 0 - 0.35 % |
Mangan | 0 - 1 % Show Material materials with Mangan of 0 - 1 % |
Molybdän | 5 - 7 % Show Material materials with Molybdän of 5 - 7 % |
Nickel | 0 - 0.5 % Show Material materials with Nickel of 0 - 0.5 % |
Phosphor | 0 - 0.02 % Show Material materials with Phosphor of 0 - 0.02 % |
Schwefel | 0 - 0.01 % Show Material materials with Schwefel of 0 - 0.01 % |
Silizium | 0 - 1 % Show Material materials with Silizium of 0 - 1 % |
Stickstoff | 0 - 0.25 % Show Material materials with Stickstoff of 0 - 0.25 % |
Titan | 0 - 0.1 % Show Material materials with Titan of 0 - 0.1 % |
Wolfram | 0 - 0.2 % Show Material materials with Wolfram of 0 - 0.2 % |