Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 1.9 g/cm³ Show Material materials with Dichte of 1.9 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 13 % Show Material materials with Dehnung of 13 % | |
Elastizitätsmodul | 23.0 °C | 45 GPa Show Material materials with Elastizitätsmodul of 45 GPa | |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Magnesium |
Schubmodule | 23.0 °C | 45 GPa Show Material materials with Schubmodule of 45 GPa | Typical for Magnesium |
Streckgrenze | 23.0 °C | 130 MPa Show Material materials with Streckgrenze of 130 MPa | |
Zugfestigkeit | 23.0 °C | 240 MPa Show Material materials with Zugfestigkeit of 240 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.6E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.6E-5 1/K |
Schmelzpunkt | 600 °C Show Material materials with Schmelzpunkt of 600 °C | |
Spezifische Wärmekapazität | 23.0 °C | 1040 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 1040 J/(kg·K) |
Wärmeleitfähigkeit | 23.0 °C | 72 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 72 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Aluminium | 2.4 - 3.6 % Show Material materials with Aluminium of 2.4 - 3.6 % |
Andere | 0 - 0.3 % Show Material materials with Andere of 0 - 0.3 % |
Eisen | 0 - 0.05 % Show Material materials with Eisen of 0 - 0.05 % |
Kalzium | 0 - 0.04 % Show Material materials with Kalzium of 0 - 0.04 % |
Kupfer | 0 - 0.05 % Show Material materials with Kupfer of 0 - 0.05 % |
Magnesium | 93.6 - 97.1 % Show Material materials with Magnesium of 93.6 - 97.1 % |
Mangan | 0.05 - 1 % Show Material materials with Mangan of 0.05 - 1 % |
Nickel | 0 - 5E-3 % Show Material materials with Nickel of 0 - 5E-3 % |
Silizium | 0 - 0.1 % Show Material materials with Silizium of 0 - 0.1 % |
Zink | 0.5 - 1.5 % Show Material materials with Zink of 0.5 - 1.5 % |