Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 1.9 g/cm³ Show Material materials with Dichte of 1.9 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 8.5 % Show Material materials with Dehnung of 8.5 % | |
Elastizitätsmodul | 23.0 °C | 47 GPa Show Material materials with Elastizitätsmodul of 47 GPa | |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Magnesium |
Schubmodule | 23.0 °C | 45 GPa Show Material materials with Schubmodule of 45 GPa | Typical for Magnesium |
Streckgrenze | 23.0 °C | 230 MPa Show Material materials with Streckgrenze of 230 MPa | |
Zugfestigkeit | 23.0 °C | 320 MPa Show Material materials with Zugfestigkeit of 320 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.6E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.6E-5 1/K | |
Schmelzpunkt | 650 °C Show Material materials with Schmelzpunkt of 650 °C | Typical for Magnesium | |
Spezifische Wärmekapazität | 23.0 °C | 1050 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 1050 J/(kg·K) | |
Wärmeleitfähigkeit | 23.0 °C | 52 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 52 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Aluminium | 7.8 - 9.2 % Show Material materials with Aluminium of 7.8 - 9.2 % |
Andere | 0 - 0.3 % Show Material materials with Andere of 0 - 0.3 % |
Eisen | 0 - 5E-3 % Show Material materials with Eisen of 0 - 5E-3 % |
Kupfer | 0 - 0.05 % Show Material materials with Kupfer of 0 - 0.05 % |
Magnesium | 89 - 91.9 % Show Material materials with Magnesium of 89 - 91.9 % |
Mangan | 0.12 - 0.5 % Show Material materials with Mangan of 0.12 - 0.5 % |
Nickel | 0 - 5E-3 % Show Material materials with Nickel of 0 - 5E-3 % |
Silizium | 0 - 0.1 % Show Material materials with Silizium of 0 - 0.1 % |
Zink | 0.2 - 0.8 % Show Material materials with Zink of 0.2 - 0.8 % |