Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.3 g/cm³ Show Material materials with Dichte of 8.3 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 19 % Show Material materials with Dehnung of 19 % |
Elastizitätsmodul | 23.0 °C | 200 GPa Show Material materials with Elastizitätsmodul of 200 GPa |
Streckgrenze | 23.0 °C | 1330 MPa Show Material materials with Streckgrenze of 1330 MPa |
Zugfestigkeit | 23.0 °C | 1530 MPa Show Material materials with Zugfestigkeit of 1530 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.3E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.3E-5 1/K |
Schmelzpunkt | 1260 °C Show Material materials with Schmelzpunkt of 1260 °C | |
Spezifische Wärmekapazität | 23.0 °C | 440 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 440 J/(kg·K) |
Wärmeleitfähigkeit | 23.0 °C | 11 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 11 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.2 - 0.8 % Show Material materials with Aluminium of 0.2 - 0.8 % |
Bor | 0 - 6E-3 % Show Material materials with Bor of 0 - 6E-3 % |
Chrom | 17 - 21 % Show Material materials with Chrom of 17 - 21 % |
Eisen | 11.1 - 24.6 % Show Material materials with Eisen of 11.1 - 24.6 % |
Kobalt | 0 - 1 % Show Material materials with Kobalt of 0 - 1 % |
Kohlenstoff | 0 - 0.08 % Show Material materials with Kohlenstoff of 0 - 0.08 % |
Kupfer | 0 - 0.3 % Show Material materials with Kupfer of 0 - 0.3 % |
Mangan | 0 - 0.35 % Show Material materials with Mangan of 0 - 0.35 % |
Molybdän | 2.8 - 3.3 % Show Material materials with Molybdän of 2.8 - 3.3 % |
Nickel | 50 - 55 % Show Material materials with Nickel of 50 - 55 % |
Niobium | 4.8 - 5.5 % Show Material materials with Niobium of 4.8 - 5.5 % |
Phosphor | 0 - 0.02 % Show Material materials with Phosphor of 0 - 0.02 % |
Schwefel | 0 - 0.015 % Show Material materials with Schwefel of 0 - 0.015 % |
Silizium | 0 - 0.35 % Show Material materials with Silizium of 0 - 0.35 % |
Titan | 0.65 - 1.2 % Show Material materials with Titan of 0.65 - 1.2 % |