Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 10 g/cm³ Show Material materials with Dichte of 10 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 1.2 % Show Material materials with Dehnung of 1.2 % | |
Elastizitätsmodul | 23.0 °C | 86 GPa Show Material materials with Elastizitätsmodul of 86 GPa | |
Poissonzahl | 23.0 °C | 0.37 [-] Show Material materials with Poissonzahl of 0.37 [-] | Typical for Silver |
Schubmodule | 23.0 °C | 30 GPa Show Material materials with Schubmodule of 30 GPa | Typical for Silver |
Zugfestigkeit | 23.0 °C | 460 MPa Show Material materials with Zugfestigkeit of 460 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.9E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.9E-5 1/K | |
Schmelzpunkt | 780 °C Show Material materials with Schmelzpunkt of 780 °C | ||
Spezifische Wärmekapazität | 23.0 °C | 250 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 250 J/(kg·K) | |
Wärmeleitfähigkeit | 23.0 °C | 417 - 428 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 417 - 428 W/(m·K) | Typical for Silver |
Chemical properties
Property | Value |
---|---|
Aluminium | 0 - 5E-3 % Show Material materials with Aluminium of 0 - 5E-3 % |
Andere | 0 - 0.06 % Show Material materials with Andere of 0 - 0.06 % |
Blei | 0 - 0.03 % Show Material materials with Blei of 0 - 0.03 % |
Cadmium | 0 - 0.05 % Show Material materials with Cadmium of 0 - 0.05 % |
Eisen | 0 - 0.05 % Show Material materials with Eisen of 0 - 0.05 % |
Kupfer | 9 - 10.4 % Show Material materials with Kupfer of 9 - 10.4 % |
Nickel | 0 - 0.01 % Show Material materials with Nickel of 0 - 0.01 % |
Phosphor | 0 - 0.02 % Show Material materials with Phosphor of 0 - 0.02 % |
Silber | 89.6 - 91 % Show Material materials with Silber of 89.6 - 91 % |
Zink | 0 - 0.06 % Show Material materials with Zink of 0 - 0.06 % |