Allgemein
Property | Value | Condition | Related Standards |
---|---|---|---|
Dichte | 2.7 g/cm³ Show Material materials with Dichte of 2.7 g/cm³ | H16 | |
2.705 g/cm³ Show Material materials with Dichte of 2.705 g/cm³ | H16 | AA Standards |
Mechanisch
Property | Value | Condition | Related Standards | Comment |
---|---|---|---|---|
Elastizitätsmodul | 69.0 GPa Show Material materials with Elastizitätsmodul of 69.0 GPa | H16 | AA Standards | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 1000 Series Aluminium | ||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 1000 Series Aluminium | ||
Schubmodule | 25.9 GPa Show Material materials with Schubmodule of 25.9 GPa | Typical for Wrought 1000 Series Aluminium | ||
Streckgrenze | 110.0 MPa Show Material materials with Streckgrenze of 110.0 MPa | H16 | AA Standards | RP02 |
110.0 MPa Show Material materials with Streckgrenze of 110.0 MPa | H16 | |||
Zugfestigkeit | 120.0 MPa Show Material materials with Zugfestigkeit of 120.0 MPa | H16 | ||
125.0 MPa Show Material materials with Zugfestigkeit of 125.0 MPa | H16 | AA Standards |
Thermisch
Property | Temperature | Value | Condition | Related Standards |
---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 2.4e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.4e-05 1/K | H16 | ||
20 °C | 2.36e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.36e-05 1/K | H16 | AA Standards | |
100 °C | 2.36e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.36e-05 1/K | H16 | AA Standards | |
Schmelzpunkt | 645.0 - 655.0 °C Show Material materials with Schmelzpunkt of 645.0 - 655.0 °C | H16 | AA Standards | |
650.0 °C Show Material materials with Schmelzpunkt of 650.0 °C | H16 | |||
Spezifische Wärmekapazität | 900.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 900.0 J/(kg·K) | H16 | ||
Wärmeleitfähigkeit | 230.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 230.0 W/(m·K) | H16 | ||
234 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 234 W/(m·K) | H16 | AA Standards |
Elektrisch
Property | Value | Condition | Related Standards |
---|---|---|---|
Elektrische Leitfähigkeit | 36000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 36000000.0 S/m | H16 | AA Standards |
spezifischer Widerstand | 2.78e-08 Ω·m Show Material materials with spezifischer Widerstand of 2.78e-08 Ω·m | H16 | AA Standards |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Aluminium | 99.5 % Show Material materials with Aluminium of 99.5 % | H16 | AA Standards |
99.5 - 100.0 % Show Material materials with Aluminium of 99.5 - 100.0 % | H16 | ||
Andere | 0.1 % Show Material materials with Andere of 0.1 % | H16 | |
Bor | 0.05 % Show Material materials with Bor of 0.05 % | H16 | AA Standards |
Chrom | 0.01 % Show Material materials with Chrom of 0.01 % | H16 | AA Standards |
Eisen | 0.40 % Show Material materials with Eisen of 0.40 % | H16 | AA Standards |
0.4 % Show Material materials with Eisen of 0.4 % | H16 | ||
Gallium | 0.03 % Show Material materials with Gallium of 0.03 % | H16 | AA Standards |
Kupfer | 0.05 % Show Material materials with Kupfer of 0.05 % | H16 | AA Standards |
Mangan | 0.01 % Show Material materials with Mangan of 0.01 % | H16 | AA Standards |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % | H16 | AA Standards |
Titan | 0.02 % Show Material materials with Titan of 0.02 % | H16 | |
Vanadium | 0.02 % Show Material materials with Vanadium of 0.02 % | H16 | |
Zink | 0.05 % Show Material materials with Zink of 0.05 % | H16 | AA Standards |
Technological properties
Property | ||
---|---|---|
Brazing | general: possible with commercial processes and methods | |
Corrosion properties | Stress corrosion cracking: no damage during operation and laboratory tests, general: very good, without protection in industrial or seawater atmosphere | |
General machinability | General: not suitable (O, H12, H111), poor (H14, H24, H16, H26, H18) | |
Workability | general (condition): good (O, H12, H111, H14, H24), acceptable (H16, H26, H18) |