Allgemein
Property | Value | Condition |
---|---|---|
Dichte | 3.1 g/cm³ Show Material materials with Dichte of 3.1 g/cm³ | T6 |
Mechanisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Charpy impact energy, V-notch | 5.0 - 15.0 J Show Material materials with Charpy impact energy, V-notch of 5.0 - 15.0 J | T6 | |||
Dehnung | 4.0 % Show Material materials with Dehnung of 4.0 % | T6 | Pink Sheets, ASTM B618 | Casting | A100 |
7.2 % Show Material materials with Dehnung of 7.2 % | T6 | ||||
8 % Show Material materials with Dehnung of 8 % | T6 | Sand cast, elongation in 50 mm | |||
Elastizitätsmodul | 71.0 GPa Show Material materials with Elastizitätsmodul of 71.0 GPa | T6 | |||
71 GPa Show Material materials with Elastizitätsmodul of 71 GPa | T6 | ||||
Härte, Brinell | 135 [-] Show Material materials with Härte, Brinell of 135 [-] | T6 | 500 kg load, 10 mm b | ||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | T6 | |||
Schubmodule | 23.0 GPa Show Material materials with Schubmodule of 23.0 GPa | T6 | |||
Streckgrenze | 345.0 MPa Show Material materials with Streckgrenze of 345.0 MPa | T6 | Pink Sheets, ASTM B618 | Casting | RP02 |
379 MPa Show Material materials with Streckgrenze of 379 MPa | T6 | Sand cast, RP02 | |||
400.0 MPa Show Material materials with Streckgrenze of 400.0 MPa | T6 | ||||
Zugfestigkeit | 415.0 MPa Show Material materials with Zugfestigkeit of 415.0 MPa | T6 | Pink Sheets, ASTM B618 | Casting | |
448 MPa Show Material materials with Zugfestigkeit of 448 MPa | T6 | Sand cast | |||
460.0 MPa Show Material materials with Zugfestigkeit of 460.0 MPa | T6 |
Thermisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 2.1e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.1e-05 1/K | T6 | ||||
100 °C | 0.0000193 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 0.0000193 1/K | T6 | unstated value between 20°C and the mentioned temperature | |||
200 °C | 0.0000227 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 0.0000227 1/K | T6 | unstated value between 20°C and the mentioned temperature | |||
300 °C | 0.0000247 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 0.0000247 1/K | T6 | unstated value between 20°C and the mentioned temperature | |||
Schmelzpunkt | 570.0 °C Show Material materials with Schmelzpunkt of 570.0 °C | T6 | ||||
571.0 - 649.0 °C Show Material materials with Schmelzpunkt of 571.0 - 649.0 °C | T6 | Pink Sheets, ASTM B618 | Casting | |||
Spezifische Wärmekapazität | 920.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 920.0 J/(kg·K) | T6 | ||||
Wärmeleitfähigkeit | 120.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 120.0 W/(m·K) | T6 |
Elektrisch
Property | Value | Condition | Comment |
---|---|---|---|
Elektrische Leitfähigkeit | 16000000.0 - 19000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 16000000.0 - 19000000.0 S/m | T6 | Typical/Derived values |
Specific Electrical conductivity | 27.0 - 32.0 % IACS Show Material materials with Specific Electrical conductivity of 27.0 - 32.0 % IACS | T6 | Typical values |
spezifischer Widerstand | 5.4e-08 - 6.4e-08 Ω·m Show Material materials with spezifischer Widerstand of 5.4e-08 - 6.4e-08 Ω·m | T6 | Typical values |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminium | 92.1 - 95.1 % Show Material materials with Aluminium of 92.1 - 95.1 % | T6 | ||
Andere | 0.1 % Show Material materials with Andere of 0.1 % | T6 | ||
Eisen | 0.15 % Show Material materials with Eisen of 0.15 % | T6 | ||
0.15 % Show Material materials with Eisen of 0.15 % | T6 | Pink Sheets, ASTM B618 | Casting | |
Kupfer | 4.0 - 5.2 % Show Material materials with Kupfer of 4.0 - 5.2 % | T6 | Pink Sheets, ASTM B618 | Casting |
Magnesium | 0.15 - 0.55 % Show Material materials with Magnesium of 0.15 - 0.55 % | T6 | Pink Sheets, ASTM B618 | Casting |
Mangan | 0.2 - 0.5 % Show Material materials with Mangan of 0.2 - 0.5 % | T6 | Pink Sheets, ASTM B618 | Casting |
Silber | 0.4 - 1.0 % Show Material materials with Silber of 0.4 - 1.0 % | T6 | Pink Sheets, ASTM B618 | Casting |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % | T6 | Pink Sheets, ASTM B618 | Casting |
Titan | 0.15 - 0.35 % Show Material materials with Titan of 0.15 - 0.35 % | T6 | Pink Sheets, ASTM B618 | Casting |