Allgemein
Property | Value | Condition |
---|---|---|
Dichte | 5.4 g/cm³ Show Material materials with Dichte of 5.4 g/cm³ | High Strength |
Mechanisch
Property | Value | Condition |
---|---|---|
Dehnung | 9.2 % Show Material materials with Dehnung of 9.2 % | High Strength |
Elastizitätsmodul | 150.0 GPa Show Material materials with Elastizitätsmodul of 150.0 GPa | High Strength |
Streckgrenze | 1180.0 MPa Show Material materials with Streckgrenze of 1180.0 MPa | High Strength |
Zugfestigkeit | 1350.0 MPa Show Material materials with Zugfestigkeit of 1350.0 MPa | High Strength |
Thermisch
Property | Value | Condition | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 1.1e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.1e-05 1/K | High Strength | |
Schmelzpunkt | 1550.0 - 1815.0 °C Show Material materials with Schmelzpunkt of 1550.0 - 1815.0 °C | Typical for Titanium Beta Alloy | |
Spezifische Wärmekapazität | 500.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 500.0 J/(kg·K) | High Strength | |
Wärmeleitfähigkeit | 6.0 - 11.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 6.0 - 11.0 W/(m·K) | Typical for Titanium Beta Alloy |
Chemical properties
Property | Value | Condition |
---|---|---|
Aluminium | 2.5 - 3.5 % Show Material materials with Aluminium of 2.5 - 3.5 % | High Strength |
Andere | 0.4 % Show Material materials with Andere of 0.4 % | High Strength |
Eisen | 0.4 % Show Material materials with Eisen of 0.4 % | High Strength |
Kohlenstoff | 0.05 % Show Material materials with Kohlenstoff of 0.05 % | High Strength |
Molybdän | 14.0 - 16.0 % Show Material materials with Molybdän of 14.0 - 16.0 % | High Strength |
Niobium | 2.2 - 3.2 % Show Material materials with Niobium of 2.2 - 3.2 % | High Strength |
Sauerstoff | 0.17 % Show Material materials with Sauerstoff of 0.17 % | High Strength |
Silizium | 0.15 - 0.25 % Show Material materials with Silizium of 0.15 - 0.25 % | High Strength |
Stickstoff | 0.03 % Show Material materials with Stickstoff of 0.03 % | High Strength |
Titan | 76.0 - 81.2 % Show Material materials with Titan of 76.0 - 81.2 % | High Strength |
Wasserstoff | 0.015 % Show Material materials with Wasserstoff of 0.015 % | High Strength |