Allgemein
Property | Value | Comment |
---|---|---|
Partikelgröße | 63000 nm Show Supplier Material materials with Partikelgröße of 63000 nm | Sieve analysis from 270 mesh to 100 mesh (typical max value, others as requested) |
Partikelgrößenbereich | 3.5 - 4 µm Show Supplier Material materials with Partikelgrößenbereich of 3.5 - 4 µm | Fisher S.S.S. (typical value, others as requested) |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Andere | 0.02 % Show Supplier Material materials with Andere of 0.02 % | total metallic impurities max. | |
Kohlenstoff | 5E-3 % Show Supplier Material materials with Kohlenstoff of 5E-3 % | max | |
Rhenium | balance | ||
Sauerstoff | 0.25 % Show Supplier Material materials with Sauerstoff of 0.25 % | max | |
Schwefel | 3E-3 % Show Supplier Material materials with Schwefel of 3E-3 % | max | |
Stickstoff | 0.01 % Show Supplier Material materials with Stickstoff of 0.01 % | max |
Technological properties
Property | ||
---|---|---|
Application areas | Common uses: As an alloy addition in superalloys; production of sheet foil, strip or wire for various industrial applications | |
Processing history | Produced by hydrogen reduction of Ammonium Perrhenate |