Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 4.2 g/cm³ Show Supplier Material materials with Dichte of 4.2 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Biegefestigkeit | 23.0 °C | 700 MPa Show Supplier Material materials with Biegefestigkeit of 700 MPa |
Elastizitätsmodul | 23.0 °C | 390 GPa Show Supplier Material materials with Elastizitätsmodul of 390 GPa |
Plane-Strain Fracture Toughnes | 23.0 °C | 7 - 9 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 7 - 9 MPa·√m |
Thermisch
Property | Temperature | Value |
---|---|---|
Wärmeleitfähigkeit | 23.0 °C | 35 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 35 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 23.0 °C | 3.15E-5 Ω·m Show Supplier Material materials with spezifischer Widerstand of 3.15E-5 Ω·m |
Technological properties
Property | ||
---|---|---|
Application areas | Typical application areas include: Cutting tool inserts, stamping tool parts, wear resistant parts |