Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 3.94 g/cm³ Show Supplier Material materials with Dichte of 3.94 g/cm³ | |
Porosität | 0 % Show Supplier Material materials with Porosität of 0 % | open porositiy |
Mechanisch
Property | Temperature | Value |
---|---|---|
Biegefestigkeit | 23.0 °C | 420 MPa Show Supplier Material materials with Biegefestigkeit of 420 MPa |
Elastizitätsmodul | 23.0 °C | 380 GPa Show Supplier Material materials with Elastizitätsmodul of 380 GPa |
Plane-Strain Fracture Toughnes | 23.0 °C | 3.8 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 3.8 MPa·√m |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 1000.0 °C | 8.5E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 8.5E-6 1/K | |
Max. Betriebstemperatur | 1750 °C Show Supplier Material materials with Max. Betriebstemperatur of 1750 °C | no load | |
Wärmeleitfähigkeit | 23.0 °C | 29 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 29 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 23.0 °C | 1.00E+11 Ω·m Show Supplier Material materials with spezifischer Widerstand of 1.00E+11 Ω·m |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 99.96 % Show Supplier Material materials with Aluminium of 99.96 % | as Al₂O₃ |
Chrom | 1E-3 % Show Supplier Material materials with Chrom of 1E-3 % | |
Eisen | 0.01 % Show Supplier Material materials with Eisen of 0.01 % | as Fe₂O₃ |
Kalzium | 1E-3 % Show Supplier Material materials with Kalzium of 1E-3 % | as CaO |
Magnesium | 3E-3 % Show Supplier Material materials with Magnesium of 3E-3 % | as MgO |
Silizium | 0.01 % Show Supplier Material materials with Silizium of 0.01 % | as SiO₂ |
Titan | 3E-3 % Show Supplier Material materials with Titan of 3E-3 % | as TiO₂ |
Zink | 5E-3 % Show Supplier Material materials with Zink of 5E-3 % |
Technological properties
Property | ||
---|---|---|
Application areas | Typical application areas include: High temperature labware, furnace construction, abrasives industry, pump & compressor industry, chemical & pharma industry |